PROCESS FOR RECOVERING URANIUM FROM URANIUM-BEARING ORES BY ACID LEACHING

The invention relates to a process for recovering uranium from uranium-bearing ores, by acid leaching. According to the invention, the process consists in enriching the uranium-bearing ore, by radiometric sorting, while removing the tailings below the 0.03% uranium content threshold, followed by wet...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: PETRESCU TEFAN, GEORGESCU PETRE DAN, AURELIAN FLORIAN, R EDULESCU ROZALIA, FILIP GHEORGHE, VASILE CONSTANTIN, PAN URU EUGENIA, IUHAS TIBERIUS FLAVIU, MUNTEAN IOAN
Format: Patent
Sprache:eng ; rum
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention relates to a process for recovering uranium from uranium-bearing ores, by acid leaching. According to the invention, the process consists in enriching the uranium-bearing ore, by radiometric sorting, while removing the tailings below the 0.03% uranium content threshold, followed by wet grinding in two stages, up to a granulation of 0.1 mm, the resulting cloudiness being thickened up to a S/L ratio of 1/1 with 1% floculant solution, followed by leaching this coudiness with sulphuric acid, in two stages, at 60A C for 4 hours/stage. The pulp obtained at first filtration is washed with half of the solution volume and of the washing water resulting from the second filtration, the second half of the solution (from second filtration) being used for repulping the pulp resulting from the first filtration, the resulting cloudiness being introduced into the second leaching stage, the uranium recovery from uranium-bearing solution resulting after the first filtration being performed by carbonating with Na2CO3 and filtering for separating the impurifying metal hydroxides, the remaining solution being enriched by ion exchange, the uranium in the eluates being precipitated as sodium diuranate, washed by settling-filtering, dried and stored. Invenţia se referă la un procedeu de recuperare a uraniului din minereuri uranifere, prin leşiere acidă. Procedeul conform invenţiei constă în îmbogăţirea minereului uranifer, prin sortare radiometrică, cu eliminarea sterilului sub pragul de 0,03% uraniu, urmată de măcinare, în stare umedă, în două trepte, până la o granulaţie de - 0,1 mm, iar tulbureala rezultată fiind îngroşată până la un raport S/L de 1/1 cu soluţie de floculant 1%, după care această tulbureală este leşiată cu acid sulfuric, în două trepte, la 60°C, timp de 4h/ treaptă. Pulpa obţinută de la prima filtrare este spălată cu jumătate din volumul soluţiei şi a apei de spălare de la filtrarea II, a doua jumătate a soluţiei (de la filtrarea II) fiind utilizată la repulparea pulpei de la filtrarea I, tulbureala rezultată fiind introdusă la treapta II de leşiere. Recuperarea uraniului din soluţia uraniferă rezultată după prima filtrare se face prin carbonatare cu Na2CO3 şi filtrare pentru separarea hidroxizilor metalelor impurificatoare, soluţia rămasă fiind îmbogăţită prin schimb ionic, uraniul din eluaţi fiind precipitat sub formă de diuranat de sodiu, spălat prin decantare-filtrare, uscat şi stocat.