PROCESS FOR PREPARING CALCIUM POLYSULPHIDE
The invention relates to a process for preparing calcium polysulphide by boiling the hydrated lime with industrial coke sulphur at 95...100°C, for 120 min. In order to prepare a concentrated calcium polysulphide solution having a total sulphur content of 15...22%, the weight ratio sulphur : lime : w...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; rum |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention relates to a process for preparing calcium polysulphide by boiling the hydrated lime with industrial coke sulphur at 95...100°C, for 120 min. In order to prepare a concentrated calcium polysulphide solution having a total sulphur content of 15...22%, the weight ratio sulphur : lime : water is of 1 : 1.05 : 7.48.
Invenţia se referă la un procedeu de obţinere a polisulfurii de calciu, prin fierberea laptelui de var timp de 120 min, la 95...100°C, cu sulf tehnic de cocserie. Pentru obţinerea unei soluţii concentrate de polisulfură de calciu, cu un conţinut de sulf total de 15...22%, raportul în greutate sulf : var : apă este de 1 : 1,05 : 7,48. |
---|