ELECTRODE FOR EROSION PROCESSING AND PRODUCTION METHOD

The spark machining electrode of reduced metal requirement comprises porous copper (93-95%), graphite (1-4%) and titanium (5-7%) prod. incorporating industrial glycerine at 8-10g per kg of its compsn. The powder constituents are sintered at 900-1030 deg. C and held for 60-165 min., prior to cooling...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: OBRETIN ALEXANDRINA, RO, MANTESCU GRIGORE, RO, BUDAU NICOLAE, RO, NICA NICOLAE, RO
Format: Patent
Sprache:eng ; rum
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The spark machining electrode of reduced metal requirement comprises porous copper (93-95%), graphite (1-4%) and titanium (5-7%) prod. incorporating industrial glycerine at 8-10g per kg of its compsn. The powder constituents are sintered at 900-1030 deg. C and held for 60-165 min., prior to cooling over 3-5 hr. The sintering is carried out in a reducing atmos. or under vacuum at 1-3 mmHg.