PROCESS FOR TREATING TRICOTS OF COTTON AND CHEMICAL FIBRES BLEND
A soaking agent, for treating knitted fabrics made with a mixt. of cotton and synthetic yarns, contains 1.2% of a mixt. of sulphated and unsulphated fatty acid, and 1-2% of a synergistic mixt. of polyoxyethylene derivs.. Treatment takes place at 40-50 deg.C. for 20-30 minutes, at a ratio of 6:1-8:1....
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; rum |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A soaking agent, for treating knitted fabrics made with a mixt. of cotton and synthetic yarns, contains 1.2% of a mixt. of sulphated and unsulphated fatty acid, and 1-2% of a synergistic mixt. of polyoxyethylene derivs.. Treatment takes place at 40-50 deg.C. for 20-30 minutes, at a ratio of 6:1-8:1. The soaked fabric is centrifuged corresponding to 70-75% wringing level; followed by drying and pressing. |
---|