BLOW MOLDING RESINS WITH IMPROVED ESCR

Polyethylene resins having improved environmental stress crack resistance, stiffness and impact resistance is made by a process comprising feeding both a chromium oxide catalyst and a silyl chromium catalyst into a polymerization reactor. The chromium oxide catalyst and the silyl chromium catalyst a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: JAKER, STEPHEN PAUL, ST. JEAN, GUYLAINE, JORGENSEN, ROBERT J, MURE, CLIFF ROBERT, BREETZ, KAREN
Format: Patent
Sprache:eng ; pol
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Polyethylene resins having improved environmental stress crack resistance, stiffness and impact resistance is made by a process comprising feeding both a chromium oxide catalyst and a silyl chromium catalyst into a polymerization reactor. The chromium oxide catalyst and the silyl chromium catalyst are on separate supports. The chromium oxide catalyst is 25-50 weight percent and the silyl chromium catalyst is 50-75 weight percent of the total weight of catalyst. The catalysts may be added separately or as a single mixture.