Process for forming polylactide expanded bead foam
Expanded poly(lactide) (PLA) beads are made by pressurizing PLA beads with carbon dioxide at approximately room temperature, heating the beads under pressure to 90 to 160C to saturate and partially crystallize the beads, and then depressurizing and cooling the beads. The PLA beads contain a blend of...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Expanded poly(lactide) (PLA) beads are made by pressurizing PLA beads with carbon dioxide at approximately room temperature, heating the beads under pressure to 90 to 160C to saturate and partially crystallize the beads, and then depressurizing and cooling the beads. The PLA beads contain a blend of PLLA and PDLA in certain ratios. The beads are useful for making expanded bead foam. |
---|