PREPARATION OF ALUMINUM CHLORHYDROXIDE HAVING A K D VALUE OF 0.4
The invention relates to a aluminum chlorhydroxide product high in molecular species content having a Kd value equal to 0.4 prepared by heating a 5 % aqueous solution of aluminum chlorhydroxide at a temperature in the range of from about 100 DEG C to about 132 DEG for a period of about 10 minutes to...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The invention relates to a aluminum chlorhydroxide product high in molecular species content having a Kd value equal to 0.4 prepared by heating a 5 % aqueous solution of aluminum chlorhydroxide at a temperature in the range of from about 100 DEG C to about 132 DEG for a period of about 10 minutes to one hour and then spray drying the product, the heating preferably being done under pressure. |
---|