FREMGANGSMAATE FOR VARMEBEHANDLING AV SILISIUM- OG KARBONHOLDIGE KERAMISKE FIBRE OG FREMSTILLING AV SLIKE FIBRE MED LAGDELT STRUKTUR
The process consists in carrying out a heat treatment under vacuum for a period of at least 3 hours and at a temperature of the order of 1000 DEG C. This treatment makes it possible to obtain fibres surrounded by a layer of endogenic SiO2 itself coated with an endogenic carbon layer. These fibres ca...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | nor |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The process consists in carrying out a heat treatment under vacuum for a period of at least 3 hours and at a temperature of the order of 1000 DEG C. This treatment makes it possible to obtain fibres surrounded by a layer of endogenic SiO2 itself coated with an endogenic carbon layer.
These fibres can be employed for the production of fibre-reinforced composite materials. |
---|