Method for and equipment for suppressing discoloration of Al-Mg products

Method and means for suppressing discoloration during thermal treatment of a product of a magnesium containing aluminium alloy, the alloy contains in wt.% Mg: 0,45 - 12,0, with a preferred range of 0,45-6,0 wt%. The product, being either an extrusion billet, a sheet ingot, a cast product, or a forge...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Øyen, Geir, Rist, Snorre, Bauger, Øystein, Steen, Idar Kjetil, Romfo, Alf Inge, Reiso, Oddvin, Pettersen, Tanja
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Method and means for suppressing discoloration during thermal treatment of a product of a magnesium containing aluminium alloy, the alloy contains in wt.% Mg: 0,45 - 12,0, with a preferred range of 0,45-6,0 wt%. The product, being either an extrusion billet, a sheet ingot, a cast product, or a forged product is heated to a temperature T where it is prone to surface discoloration and oxidation, wherein during the thermal treatment it is exposed to a suppressing atmosphere comprising 0,5-5,0% CO2gas with a preference for 0,5 - 1,5 % CO2gas.