Stål med høy varmefasthet for kjelebygging

A high-temperature steel for boiler making having improved creep strength and low tendency to hardening in welded condition, having the following melt analysis (wt. %): C 0.050 to 0.100% Si 0.15 to 0.45% Mn 0.30 to 0.70% P

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Hagen, Ingo von, Bendick, Walter, Haarmann, Klaus
Format: Patent
Sprache:nor
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A high-temperature steel for boiler making having improved creep strength and low tendency to hardening in welded condition, having the following melt analysis (wt. %): C 0.050 to 0.100% Si 0.15 to 0.45% Mn 0.30 to 0.70% P