Fremgangsmåte for fremstilling av syntetisk rutil fra en titanholdig slagg

Synthetic rutile is prepared from titaniferous slags containing alkaline-earth metal impurities, such as magnesium oxide, by a method comprising contacting the slag with chlorine at a temperature of at least about 800 DEG C., and then leaching the chlorine-treated slag with hydrochloric acid at a te...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: GUEGUIN, MICHEL
Format: Patent
Sprache:nor
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Synthetic rutile is prepared from titaniferous slags containing alkaline-earth metal impurities, such as magnesium oxide, by a method comprising contacting the slag with chlorine at a temperature of at least about 800 DEG C., and then leaching the chlorine-treated slag with hydrochloric acid at a temperature of at least about 150 DEG C.