FILLET ARC WELDED JOINT AND METHOD FOR FORMING SAME
At least one stiffening bead (32) formed by arc welding is formed on a surface of at least one metal member separately from a fillet bead (3) formed by fillet arc welding. The stiffening bead (32) is formed at an angle of 45-135° with the fillet bead (3), and is formed so as to overlap with the fill...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; spa |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | At least one stiffening bead (32) formed by arc welding is formed on a surface of at least one metal member separately from a fillet bead (3) formed by fillet arc welding. The stiffening bead (32) is formed at an angle of 45-135° with the fillet bead (3), and is formed so as to overlap with the fillet bead (3). The total (l1) of the length of the stiffening bead (32) may be at least 0.5 times the length (L) of the fillet bead (3), for example.
Al menos un cordón (32) de refuerzo está formado por la soldadura de arco sobre una superficie de al menos uno de los miembros de metal además de un cordón (3) de filete en ángulo formado por la soldadura por arco en ángulo. El cordón (32) de refuerzo está formado para tener un ángulo de 45° a 135° con respecto al cordón (3) de filete en ángulo y para solaparse con el cordón (3) de filete en ángulo. La suma total 11 de las longitudes de los cordones (32) de refuerzo puede ser, por ejemplo, 0.5 veces o más de una longitud L del cordón (3) de filete en ángulo. |
---|