AFTER-TREATMENT METHOD FOR TREATING AN ALUMINIUM DEPOSITION OF

The aftertreatment of aluminium-deposited steel plate is conducted by heat treating the plated steel plate at 450-550 deg.C for less than 2 mins, and bathing it in the distilled water at the temperature higher than 80 deg.C for more than 10 mins. The method is much simpler than the conventional chro...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SHIN, JUNG - CHOL, JUNG, JIN - HO, CHOE, JANG - HYUN, CHON, JAE - HO
Format: Patent
Sprache:eng ; kor
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The aftertreatment of aluminium-deposited steel plate is conducted by heat treating the plated steel plate at 450-550 deg.C for less than 2 mins, and bathing it in the distilled water at the temperature higher than 80 deg.C for more than 10 mins. The method is much simpler than the conventional chromate process. Aluminium-plated steel plate treated by this method has an excellent anti-corrosion property and can be used for outdoor structural material.