PROCESS FOR PRODUCING LIQUID CRYSTAL PITCH HAVING ANISOTROPY

An anisotropic liquid crystal pitch is produced by: (a) heating a raw material, which is coalic heavy oil and pitch, up to 350-410 deg.C at 3-10 deg.C/min, in inert gas of 1-100 torr, and heat treating it at 600-1000 rpm for 2-5 hours, and (b) reheating it up to 400-470 deg.C at 5-10 deg.C/min and h...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LEE, KYU - DONG, YUN, SUNG - HO, OH, SAE - MIN, PARK, YAN - DUCK
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:An anisotropic liquid crystal pitch is produced by: (a) heating a raw material, which is coalic heavy oil and pitch, up to 350-410 deg.C at 3-10 deg.C/min, in inert gas of 1-100 torr, and heat treating it at 600-1000 rpm for 2-5 hours, and (b) reheating it up to 400-470 deg.C at 5-10 deg.C/min and heat treating at more than 600 rpm in a pressure of 10-760 torr within 2 hours. Its melting temperature is less than 370 deg.C.