ACICULAR PARTICULATE MATERIAL CONTAINING IRON CARBIDE

This invention relates to a magnetic coating compsn. comprising magnetic acicular powder contg. iron carbide 20 wt.%. The ratio of length to width of the acicular porticulats is 3 to 1, average length being 0.1-2 m. Iron carbide may be Fe3C2, Fe2C, Fe20Cg (Fe22C), or a mixt. of any two of these.

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SHIBUYA, YOSHIYUKI, DAIMON, SHIGEO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:This invention relates to a magnetic coating compsn. comprising magnetic acicular powder contg. iron carbide 20 wt.%. The ratio of length to width of the acicular porticulats is 3 to 1, average length being 0.1-2 m. Iron carbide may be Fe3C2, Fe2C, Fe20Cg (Fe22C), or a mixt. of any two of these.