저합금강 단조물 생산공정

내용 없음 A forging method to obtain increased elastic limit without detriment to the elongation and the tensile strength in which a low-alloy steel with up to 0.6% carbon is subjected to forging and the entire forging operation or at least the last forging stage is effected at a temperature up to 1060...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Format: Patent
Sprache:kor
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:내용 없음 A forging method to obtain increased elastic limit without detriment to the elongation and the tensile strength in which a low-alloy steel with up to 0.6% carbon is subjected to forging and the entire forging operation or at least the last forging stage is effected at a temperature up to 1060 DEG C., any earlier forging steps being carried out at temperatures above 1100 DEG C. and up to 1250 DEG C.