METHOD FOR SURFACE MODIFYING FELT ELECTRODE FOR REDOX FLOW BATTERY
A surface modification method for a graphite felt electrode for a vanadium redox flow battery is provided. The surface modification method includes the steps of: i) forming an oxygen functional group on at least one surface of the graphite felt electrode before modifying the surface of the graphite...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; kor |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A surface modification method for a graphite felt electrode for a vanadium redox flow battery is provided. The surface modification method includes the steps of: i) forming an oxygen functional group on at least one surface of the graphite felt electrode before modifying the surface of the graphite felt electrode; and ii) heat treating at least one surface of the graphite felt electrode on which the oxygen functional group is formed at a temperature of 800 to 900 deg. C for 30 to 60 minutes in an ammonia gas atmosphere to form a nitrogen functional group. In the step of forming an oxygen functional group, the oxygen functional group is a carboxyl group (-COOH), a carbonyl group (C=O), or a hydroxyl group (-OH).
바나듐 레독스 흐름전지용 그라파이트 펠트전극의 표면 개질방법을 제공한다. 표면 개질방법은 i) 그라파이트 펠트전극 표면의 개질처리 전 그라파이트 펠트전극의 적어도 일면에 산소 작용기를 형성하는 단계, 및 ii) 산소 작용기가 형성된 그라파이트 펠트전극의 적어도 일면에 암모니아 가스 분위기 하에서 800℃ 내지 900℃의 온도로 30분 내지 60분 동안 열처리하여 질소 작용기를 형성하는 단계를 포함한다. 산소 작용기를 형성하는 단계에서, 산소 작용기는 카복실기(-COOH), 카보닐기(C=O) 또는 하이드록실기(-OH)이다. |
---|