NON-ORIENTED ELECTRICAL STEEL SHEET AND METHOD FOR MANUFACTURING THE SAME
According to an embodiment of the present invention, a non-oriented electrical steel sheet comprises: 0.005wt% or less of C (excluding 0 wt%); 1.5-3.0 wt% of Si; 0.4-1.5 wt% of Mn; 0.005 wt% or less of S (excluding 0 wt%); 0.0001-0.7 wt% of Al; 0.005 wt% or less of N (excluding 0 wt%); 0.005 wt% or...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; kor |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | According to an embodiment of the present invention, a non-oriented electrical steel sheet comprises: 0.005wt% or less of C (excluding 0 wt%); 1.5-3.0 wt% of Si; 0.4-1.5 wt% of Mn; 0.005 wt% or less of S (excluding 0 wt%); 0.0001-0.7 wt% of Al; 0.005 wt% or less of N (excluding 0 wt%); 0.005 wt% or less of Ti (excluding 0 wt%); 0.001-0.02 wt% of Cu; 0.01-0.05 wt% of Sb; 0.001-0.1 wt% of Sn; 0.005-0.07 wt% of P; and remaining Fe and other inevitable impurities. The content of Mn, Si, and Al satisfies the below [Formula 1], and the content of Sb, Sn, and P satisfies the below [Formula 2]. The number of (Mn, Cu)S precipitates with the size of 0.5 ㎛ or smaller is 1/㎛^3 or less. [Formula 1] 0.19 |
---|