METHOD FOR PREVENTING SURFACE DEFFECTS IN FLOATING FLAT GLASS, FLAT GLASS AND USE THEREOF

The invention relates to a method for preventing surface deposition and/or crater-shaped hole defects during the production of floating flat glass. Said method consists of producing a glass melt, purifying said melt and floating said purified melt on the surface of the liquid metal under an inert ga...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: BEIER WOLFRAM, DAHLMANN ULF
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator BEIER WOLFRAM
DAHLMANN ULF
description The invention relates to a method for preventing surface deposition and/or crater-shaped hole defects during the production of floating flat glass. Said method consists of producing a glass melt, purifying said melt and floating said purified melt on the surface of the liquid metal under an inert gas atmosphere. Said method is characterised in that it i) defines the hydrogen content in the inert gas to a maximum of 7 Vol. % and ii) adjusts the oxygen partial pressure in the floating gas melt a) by means of a metal, whereby the reaction enthalpy for the oxidation G° (Me /MexOy7) is >-575,8 + 0.21 T[K] or b) by means of a metal whereby the reaction enthalpy for the oxidation G° (Me /MexOy) is
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_KR20080038231A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>KR20080038231A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_KR20080038231A3</originalsourceid><addsrcrecordid>eNqNirEKwjAUALM4iPoPD1wVYrN0Dcl7TTEmkrwWnEqROIkW6v8jiIOj0x3cLcXlhOyiBYoJzgl7DNyGBnKXSBsEi0RoOEMbgHzUn0heMzRe57z7cdDBQpcR2GHCSGuxuI33uWy-XIktIRu3L9NzKPM0XsujvIZjqqSspVR1pQ5a_Xe9AalqMc8</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PREVENTING SURFACE DEFFECTS IN FLOATING FLAT GLASS, FLAT GLASS AND USE THEREOF</title><source>esp@cenet</source><creator>BEIER WOLFRAM ; DAHLMANN ULF</creator><creatorcontrib>BEIER WOLFRAM ; DAHLMANN ULF</creatorcontrib><description>The invention relates to a method for preventing surface deposition and/or crater-shaped hole defects during the production of floating flat glass. Said method consists of producing a glass melt, purifying said melt and floating said purified melt on the surface of the liquid metal under an inert gas atmosphere. Said method is characterised in that it i) defines the hydrogen content in the inert gas to a maximum of 7 Vol. % and ii) adjusts the oxygen partial pressure in the floating gas melt a) by means of a metal, whereby the reaction enthalpy for the oxidation G° (Me /MexOy7) is &gt;-575,8 + 0.21 T[K] or b) by means of a metal whereby the reaction enthalpy for the oxidation G° (Me /MexOy) is &lt;-575.8 + 0.21 T[K].</description><language>eng</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2008</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20080502&amp;DB=EPODOC&amp;CC=KR&amp;NR=20080038231A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20080502&amp;DB=EPODOC&amp;CC=KR&amp;NR=20080038231A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>BEIER WOLFRAM</creatorcontrib><creatorcontrib>DAHLMANN ULF</creatorcontrib><title>METHOD FOR PREVENTING SURFACE DEFFECTS IN FLOATING FLAT GLASS, FLAT GLASS AND USE THEREOF</title><description>The invention relates to a method for preventing surface deposition and/or crater-shaped hole defects during the production of floating flat glass. Said method consists of producing a glass melt, purifying said melt and floating said purified melt on the surface of the liquid metal under an inert gas atmosphere. Said method is characterised in that it i) defines the hydrogen content in the inert gas to a maximum of 7 Vol. % and ii) adjusts the oxygen partial pressure in the floating gas melt a) by means of a metal, whereby the reaction enthalpy for the oxidation G° (Me /MexOy7) is &gt;-575,8 + 0.21 T[K] or b) by means of a metal whereby the reaction enthalpy for the oxidation G° (Me /MexOy) is &lt;-575.8 + 0.21 T[K].</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2008</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNirEKwjAUALM4iPoPD1wVYrN0Dcl7TTEmkrwWnEqROIkW6v8jiIOj0x3cLcXlhOyiBYoJzgl7DNyGBnKXSBsEi0RoOEMbgHzUn0heMzRe57z7cdDBQpcR2GHCSGuxuI33uWy-XIktIRu3L9NzKPM0XsujvIZjqqSspVR1pQ5a_Xe9AalqMc8</recordid><startdate>20080502</startdate><enddate>20080502</enddate><creator>BEIER WOLFRAM</creator><creator>DAHLMANN ULF</creator><scope>EVB</scope></search><sort><creationdate>20080502</creationdate><title>METHOD FOR PREVENTING SURFACE DEFFECTS IN FLOATING FLAT GLASS, FLAT GLASS AND USE THEREOF</title><author>BEIER WOLFRAM ; DAHLMANN ULF</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_KR20080038231A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2008</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>BEIER WOLFRAM</creatorcontrib><creatorcontrib>DAHLMANN ULF</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>BEIER WOLFRAM</au><au>DAHLMANN ULF</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PREVENTING SURFACE DEFFECTS IN FLOATING FLAT GLASS, FLAT GLASS AND USE THEREOF</title><date>2008-05-02</date><risdate>2008</risdate><abstract>The invention relates to a method for preventing surface deposition and/or crater-shaped hole defects during the production of floating flat glass. Said method consists of producing a glass melt, purifying said melt and floating said purified melt on the surface of the liquid metal under an inert gas atmosphere. Said method is characterised in that it i) defines the hydrogen content in the inert gas to a maximum of 7 Vol. % and ii) adjusts the oxygen partial pressure in the floating gas melt a) by means of a metal, whereby the reaction enthalpy for the oxidation G° (Me /MexOy7) is &gt;-575,8 + 0.21 T[K] or b) by means of a metal whereby the reaction enthalpy for the oxidation G° (Me /MexOy) is &lt;-575.8 + 0.21 T[K].</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_KR20080038231A
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
METALLURGY
MINERAL OR SLAG WOOL
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title METHOD FOR PREVENTING SURFACE DEFFECTS IN FLOATING FLAT GLASS, FLAT GLASS AND USE THEREOF
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-30T01%3A51%3A30IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=BEIER%20WOLFRAM&rft.date=2008-05-02&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EKR20080038231A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true