METHOD FOR PREVENTING SURFACE DEFFECTS IN FLOATING FLAT GLASS, FLAT GLASS AND USE THEREOF

The invention relates to a method for preventing surface deposition and/or crater-shaped hole defects during the production of floating flat glass. Said method consists of producing a glass melt, purifying said melt and floating said purified melt on the surface of the liquid metal under an inert ga...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: BEIER WOLFRAM, DAHLMANN ULF
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention relates to a method for preventing surface deposition and/or crater-shaped hole defects during the production of floating flat glass. Said method consists of producing a glass melt, purifying said melt and floating said purified melt on the surface of the liquid metal under an inert gas atmosphere. Said method is characterised in that it i) defines the hydrogen content in the inert gas to a maximum of 7 Vol. % and ii) adjusts the oxygen partial pressure in the floating gas melt a) by means of a metal, whereby the reaction enthalpy for the oxidation G° (Me /MexOy7) is >-575,8 + 0.21 T[K] or b) by means of a metal whereby the reaction enthalpy for the oxidation G° (Me /MexOy) is