COLORED COMPOSITION AND COLOR FILTER USING THE SAME

A colored composition is provided to reduce observable defects on coating film when applied to a spin coating method or die coating method, and to produce a good quality of color filters by forming a filter segment and/or black matrix with almost invisible film defects. The colored composition conta...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ASAHI NORIKO, FUJITA KENICHI, AMASAKI TADASU, YAMADA KAZUNORI, WAKU TOSHIO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ASAHI NORIKO
FUJITA KENICHI
AMASAKI TADASU
YAMADA KAZUNORI
WAKU TOSHIO
description A colored composition is provided to reduce observable defects on coating film when applied to a spin coating method or die coating method, and to produce a good quality of color filters by forming a filter segment and/or black matrix with almost invisible film defects. The colored composition contains a colorant carrier consisting of a transparent resin, a precursor thereof, or a mixture thereof, a colorant, an organic solvent, and a surface tension-adjusting agent. According to a Wilhelmy plate method, when a glass plate 22mm wide, 22mm long, and 0.145mm high is dipped in the colored composition to a depth of 2.5mm in such a direction that one side of the glass plate is perpendicular to the liquid surface of the composition, force A(at 25°C) measured when the glass plate is stationary is 1.16mN or more, and force A' and force B(measured at 25°C) satisfy the following relation of 0.08
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_KR20070062938A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>KR20070062938A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_KR20070062938A3</originalsourceid><addsrcrecordid>eNrjZDB29vfxD3J1UXD29w3wD_YM8fT3U3D0A_GB4gpunj4hrkEKocGefu4KIR6uCsGOvq48DKxpiTnFqbxQmptB2c01xNlDN7UgPz61uCAxOTUvtSTeO8jIwMDcwMDMyNLYwtGYOFUAMoEn4Q</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>COLORED COMPOSITION AND COLOR FILTER USING THE SAME</title><source>esp@cenet</source><creator>ASAHI NORIKO ; FUJITA KENICHI ; AMASAKI TADASU ; YAMADA KAZUNORI ; WAKU TOSHIO</creator><creatorcontrib>ASAHI NORIKO ; FUJITA KENICHI ; AMASAKI TADASU ; YAMADA KAZUNORI ; WAKU TOSHIO</creatorcontrib><description>A colored composition is provided to reduce observable defects on coating film when applied to a spin coating method or die coating method, and to produce a good quality of color filters by forming a filter segment and/or black matrix with almost invisible film defects. The colored composition contains a colorant carrier consisting of a transparent resin, a precursor thereof, or a mixture thereof, a colorant, an organic solvent, and a surface tension-adjusting agent. According to a Wilhelmy plate method, when a glass plate 22mm wide, 22mm long, and 0.145mm high is dipped in the colored composition to a depth of 2.5mm in such a direction that one side of the glass plate is perpendicular to the liquid surface of the composition, force A(at 25°C) measured when the glass plate is stationary is 1.16mN or more, and force A' and force B(measured at 25°C) satisfy the following relation of 0.08&lt;=B-A'&lt;=0.18. The force A' is obtained by subtracting the buoyant force of the glass plate in the colored composition from the force A. The force B is a force measured at the same moment that the glass plate is separated from the colored composition when the dipped glass plate is raised up at a speed of 2.5mm/sec in a vertical direction.</description><language>eng</language><subject>ADHESIVES ; CHEMISTRY ; DYES ; LAKES ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; MORDANTS ; NATURAL RESINS ; OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS ; OPTICS ; ORGANIC DYES OR CLOSELY-RELATED COMPOUNDS FOR PRODUCING DYES ; PAINTS ; PHYSICS ; POLISHES</subject><creationdate>2007</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20070618&amp;DB=EPODOC&amp;CC=KR&amp;NR=20070062938A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20070618&amp;DB=EPODOC&amp;CC=KR&amp;NR=20070062938A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ASAHI NORIKO</creatorcontrib><creatorcontrib>FUJITA KENICHI</creatorcontrib><creatorcontrib>AMASAKI TADASU</creatorcontrib><creatorcontrib>YAMADA KAZUNORI</creatorcontrib><creatorcontrib>WAKU TOSHIO</creatorcontrib><title>COLORED COMPOSITION AND COLOR FILTER USING THE SAME</title><description>A colored composition is provided to reduce observable defects on coating film when applied to a spin coating method or die coating method, and to produce a good quality of color filters by forming a filter segment and/or black matrix with almost invisible film defects. The colored composition contains a colorant carrier consisting of a transparent resin, a precursor thereof, or a mixture thereof, a colorant, an organic solvent, and a surface tension-adjusting agent. According to a Wilhelmy plate method, when a glass plate 22mm wide, 22mm long, and 0.145mm high is dipped in the colored composition to a depth of 2.5mm in such a direction that one side of the glass plate is perpendicular to the liquid surface of the composition, force A(at 25°C) measured when the glass plate is stationary is 1.16mN or more, and force A' and force B(measured at 25°C) satisfy the following relation of 0.08&lt;=B-A'&lt;=0.18. The force A' is obtained by subtracting the buoyant force of the glass plate in the colored composition from the force A. The force B is a force measured at the same moment that the glass plate is separated from the colored composition when the dipped glass plate is raised up at a speed of 2.5mm/sec in a vertical direction.</description><subject>ADHESIVES</subject><subject>CHEMISTRY</subject><subject>DYES</subject><subject>LAKES</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>MORDANTS</subject><subject>NATURAL RESINS</subject><subject>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</subject><subject>OPTICS</subject><subject>ORGANIC DYES OR CLOSELY-RELATED COMPOUNDS FOR PRODUCING DYES</subject><subject>PAINTS</subject><subject>PHYSICS</subject><subject>POLISHES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2007</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDB29vfxD3J1UXD29w3wD_YM8fT3U3D0A_GB4gpunj4hrkEKocGefu4KIR6uCsGOvq48DKxpiTnFqbxQmptB2c01xNlDN7UgPz61uCAxOTUvtSTeO8jIwMDcwMDMyNLYwtGYOFUAMoEn4Q</recordid><startdate>20070618</startdate><enddate>20070618</enddate><creator>ASAHI NORIKO</creator><creator>FUJITA KENICHI</creator><creator>AMASAKI TADASU</creator><creator>YAMADA KAZUNORI</creator><creator>WAKU TOSHIO</creator><scope>EVB</scope></search><sort><creationdate>20070618</creationdate><title>COLORED COMPOSITION AND COLOR FILTER USING THE SAME</title><author>ASAHI NORIKO ; FUJITA KENICHI ; AMASAKI TADASU ; YAMADA KAZUNORI ; WAKU TOSHIO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_KR20070062938A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2007</creationdate><topic>ADHESIVES</topic><topic>CHEMISTRY</topic><topic>DYES</topic><topic>LAKES</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>MORDANTS</topic><topic>NATURAL RESINS</topic><topic>OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS</topic><topic>OPTICS</topic><topic>ORGANIC DYES OR CLOSELY-RELATED COMPOUNDS FOR PRODUCING DYES</topic><topic>PAINTS</topic><topic>PHYSICS</topic><topic>POLISHES</topic><toplevel>online_resources</toplevel><creatorcontrib>ASAHI NORIKO</creatorcontrib><creatorcontrib>FUJITA KENICHI</creatorcontrib><creatorcontrib>AMASAKI TADASU</creatorcontrib><creatorcontrib>YAMADA KAZUNORI</creatorcontrib><creatorcontrib>WAKU TOSHIO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ASAHI NORIKO</au><au>FUJITA KENICHI</au><au>AMASAKI TADASU</au><au>YAMADA KAZUNORI</au><au>WAKU TOSHIO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>COLORED COMPOSITION AND COLOR FILTER USING THE SAME</title><date>2007-06-18</date><risdate>2007</risdate><abstract>A colored composition is provided to reduce observable defects on coating film when applied to a spin coating method or die coating method, and to produce a good quality of color filters by forming a filter segment and/or black matrix with almost invisible film defects. The colored composition contains a colorant carrier consisting of a transparent resin, a precursor thereof, or a mixture thereof, a colorant, an organic solvent, and a surface tension-adjusting agent. According to a Wilhelmy plate method, when a glass plate 22mm wide, 22mm long, and 0.145mm high is dipped in the colored composition to a depth of 2.5mm in such a direction that one side of the glass plate is perpendicular to the liquid surface of the composition, force A(at 25°C) measured when the glass plate is stationary is 1.16mN or more, and force A' and force B(measured at 25°C) satisfy the following relation of 0.08&lt;=B-A'&lt;=0.18. The force A' is obtained by subtracting the buoyant force of the glass plate in the colored composition from the force A. The force B is a force measured at the same moment that the glass plate is separated from the colored composition when the dipped glass plate is raised up at a speed of 2.5mm/sec in a vertical direction.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_KR20070062938A
source esp@cenet
subjects ADHESIVES
CHEMISTRY
DYES
LAKES
METALLURGY
MISCELLANEOUS APPLICATIONS OF MATERIALS
MISCELLANEOUS COMPOSITIONS
MORDANTS
NATURAL RESINS
OPTICAL ELEMENTS, SYSTEMS, OR APPARATUS
OPTICS
ORGANIC DYES OR CLOSELY-RELATED COMPOUNDS FOR PRODUCING DYES
PAINTS
PHYSICS
POLISHES
title COLORED COMPOSITION AND COLOR FILTER USING THE SAME
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-16T00%3A38%3A58IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ASAHI%20NORIKO&rft.date=2007-06-18&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EKR20070062938A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true