PROCESS FOR PRODUCING OPTICAL FILM
PROBLEM TO BE SOLVED: To provide a manufacturing method of an optical film, with which manufacturing efficiency and yield, when manufacturing a thin optical film comprising a liquid crystal substance layer without support substrate can be significantly improved. SOLUTION: In the manufacturing method...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To provide a manufacturing method of an optical film, with which manufacturing efficiency and yield, when manufacturing a thin optical film comprising a liquid crystal substance layer without support substrate can be significantly improved. SOLUTION: In the manufacturing method of the optical film, half-cutting is performed to a laminated film which is constituted by laminating a repeelable film/ a hardened acrylic resin layer/ the liquid crystal substance layer with fixed alignment/ a hardened acrylic resin layer/ an adhesive layer/ a separator film, in this order. Then the repeelable film is peeled off. COPYRIGHT: (C)2007,JPO&INPIT |
---|