TI3ALC2 COMPOSITE MATERIALS WITH HIGH STRENGTH AND MANUFACTURING PROCESS OF THE SAME
A high intensity of Ti3AlC2 is provided to have destructive strength measured by a three-point bending strength test method over 7000 MPa and to maintain excellent machinability, excellent thermal characteristic and excellent electrical characteristic. A high intensity of Ti3AlC2 composite includes...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A high intensity of Ti3AlC2 is provided to have destructive strength measured by a three-point bending strength test method over 7000 MPa and to maintain excellent machinability, excellent thermal characteristic and excellent electrical characteristic. A high intensity of Ti3AlC2 composite includes Ti3AlC2, Ti2AlC and TiCy(y>0.6) to main crystal phase. The TiCy phase less than 100 nano size is strengthened in a Ti3AlC2 matrix phase. A content of Ti2AlC secondary phase included in the Ti3AlC2 matrix phase and non-reactive TiCy(y>0.6) is 10 volume % or less. A mean size of the Ti3AlC2 grain is 30 mum or less. |
---|