PRODUCTION OF HIGH STRENGTH SIC SINTERED BODY
PURPOSE:To obtain a high strength SiC sintered body nearly free from voids by granulating and molding SiC powder having a specified particle size and a specified ratio of the major axis size to the minor axis size, sintering the molded body and impregnating Si into the sintered body. CONSTITUTION:Si...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PURPOSE:To obtain a high strength SiC sintered body nearly free from voids by granulating and molding SiC powder having a specified particle size and a specified ratio of the major axis size to the minor axis size, sintering the molded body and impregnating Si into the sintered body. CONSTITUTION:SiC powder having 10-250mum particle size and 1.0-1.2 ratio of the major axis size to the minor axis size is granulated. The granulated powder is compacted in a mold or the like and sintered in an inert gaseous atmosphere or the like. The sintered body and Si powder are put in a quartz glass vessel or the like and Si is impregnated into the sintered body. The pref. particle size of the granulated SiC powder as starting material is |
---|