JPS6217615B

By blending 5-40 parts by weight of a polyisoprene having an intrinsic viscosity [n] of 0.2-1.5 dl/g as measured in toluene at 30 DEG C. and a total 1,2- and 3,4-configuration content of 30% or less in its micro-structure into 100 parts by weight of an ethylene-propylene rubber, the adhesive propert...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: AKYAMA TAKESHI, NAGASAWA MICHIO, KOIDE TOSHUKI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:By blending 5-40 parts by weight of a polyisoprene having an intrinsic viscosity [n] of 0.2-1.5 dl/g as measured in toluene at 30 DEG C. and a total 1,2- and 3,4-configuration content of 30% or less in its micro-structure into 100 parts by weight of an ethylene-propylene rubber, the adhesive property of the ethylene-propylene rubber to fibers can be improved while maintaining the heat resistance, weather resistance, ozone resistance, low temperature properties, electrical insulating property and chemical resistance which are all characteristic of ethylene-propylene rubber.