PRODUCTION OF CHROME-CONTAINING COKE

PURPOSE:To obtain chrome-contg. coke with a reduced amt. of consumed coke, excellent heat economy and productivity, by blending a chrome ore in a powdery form and a particular reaction promoter with a raw material for production of coke and carbonizing the blend. CONSTITUTION:A raw material (A) for...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YANAGAWA TOSHIO, FUKUDA TOMIYA
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YANAGAWA TOSHIO
FUKUDA TOMIYA
description PURPOSE:To obtain chrome-contg. coke with a reduced amt. of consumed coke, excellent heat economy and productivity, by blending a chrome ore in a powdery form and a particular reaction promoter with a raw material for production of coke and carbonizing the blend. CONSTITUTION:A raw material (A) for production of coke is blended with 45wt% or more chrome ore (B) in a powdery form from which coarse grains has been removed by sieving or pulverization and 0.1wt% or more at least one reaction promoter (C) selected from among an oxide, hydroxide, carbonate and borate of an alkali metal, an oxide, hydroxide and carbonate of boron and a fluoride of an alkaline earth metal to obtain a blend. Optionally, according to need, the blend is further blended with a binder such as PVA and molded into a shaped article. The blend or shaped article is put into a coke oven and heated at, e.g., 1,150-1,200 deg.C so as to effect reduction of the chrome component to a total conversion to metal of about 50%. Thus, the desired chrome-contg. coke is obtd.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPS62174291A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPS62174291A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPS62174291A3</originalsourceid><addsrcrecordid>eNrjZFAJCPJ3CXUO8fT3U_B3U3D2CPL3ddV19vcLcfT08_RzV3D293blYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxXgHBZkaG5iZGloaOxsSoAQCKHSNW</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PRODUCTION OF CHROME-CONTAINING COKE</title><source>esp@cenet</source><creator>YANAGAWA TOSHIO ; FUKUDA TOMIYA</creator><creatorcontrib>YANAGAWA TOSHIO ; FUKUDA TOMIYA</creatorcontrib><description>PURPOSE:To obtain chrome-contg. coke with a reduced amt. of consumed coke, excellent heat economy and productivity, by blending a chrome ore in a powdery form and a particular reaction promoter with a raw material for production of coke and carbonizing the blend. CONSTITUTION:A raw material (A) for production of coke is blended with 45wt% or more chrome ore (B) in a powdery form from which coarse grains has been removed by sieving or pulverization and 0.1wt% or more at least one reaction promoter (C) selected from among an oxide, hydroxide, carbonate and borate of an alkali metal, an oxide, hydroxide and carbonate of boron and a fluoride of an alkaline earth metal to obtain a blend. Optionally, according to need, the blend is further blended with a binder such as PVA and molded into a shaped article. The blend or shaped article is put into a coke oven and heated at, e.g., 1,150-1,200 deg.C so as to effect reduction of the chrome component to a total conversion to metal of about 50%. Thus, the desired chrome-contg. coke is obtd.</description><language>eng</language><subject>CHEMISTRY ; DESTRUCTIVE DISTILLATION OF CARBONAGEOUS MATERIALS FORPRODUCTION OF GAS, COKE, TAR, OR SIMILAR MATERIALS ; FUELS ; LUBRICANTS ; METALLURGY ; PEAT ; PETROLEUM, GAS OR COKE INDUSTRIES ; TECHNICAL GASES CONTAINING CARBON MONOXIDE</subject><creationdate>1987</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19870731&amp;DB=EPODOC&amp;CC=JP&amp;NR=S62174291A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19870731&amp;DB=EPODOC&amp;CC=JP&amp;NR=S62174291A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YANAGAWA TOSHIO</creatorcontrib><creatorcontrib>FUKUDA TOMIYA</creatorcontrib><title>PRODUCTION OF CHROME-CONTAINING COKE</title><description>PURPOSE:To obtain chrome-contg. coke with a reduced amt. of consumed coke, excellent heat economy and productivity, by blending a chrome ore in a powdery form and a particular reaction promoter with a raw material for production of coke and carbonizing the blend. CONSTITUTION:A raw material (A) for production of coke is blended with 45wt% or more chrome ore (B) in a powdery form from which coarse grains has been removed by sieving or pulverization and 0.1wt% or more at least one reaction promoter (C) selected from among an oxide, hydroxide, carbonate and borate of an alkali metal, an oxide, hydroxide and carbonate of boron and a fluoride of an alkaline earth metal to obtain a blend. Optionally, according to need, the blend is further blended with a binder such as PVA and molded into a shaped article. The blend or shaped article is put into a coke oven and heated at, e.g., 1,150-1,200 deg.C so as to effect reduction of the chrome component to a total conversion to metal of about 50%. Thus, the desired chrome-contg. coke is obtd.</description><subject>CHEMISTRY</subject><subject>DESTRUCTIVE DISTILLATION OF CARBONAGEOUS MATERIALS FORPRODUCTION OF GAS, COKE, TAR, OR SIMILAR MATERIALS</subject><subject>FUELS</subject><subject>LUBRICANTS</subject><subject>METALLURGY</subject><subject>PEAT</subject><subject>PETROLEUM, GAS OR COKE INDUSTRIES</subject><subject>TECHNICAL GASES CONTAINING CARBON MONOXIDE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1987</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFAJCPJ3CXUO8fT3U_B3U3D2CPL3ddV19vcLcfT08_RzV3D293blYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxXgHBZkaG5iZGloaOxsSoAQCKHSNW</recordid><startdate>19870731</startdate><enddate>19870731</enddate><creator>YANAGAWA TOSHIO</creator><creator>FUKUDA TOMIYA</creator><scope>EVB</scope></search><sort><creationdate>19870731</creationdate><title>PRODUCTION OF CHROME-CONTAINING COKE</title><author>YANAGAWA TOSHIO ; FUKUDA TOMIYA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPS62174291A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1987</creationdate><topic>CHEMISTRY</topic><topic>DESTRUCTIVE DISTILLATION OF CARBONAGEOUS MATERIALS FORPRODUCTION OF GAS, COKE, TAR, OR SIMILAR MATERIALS</topic><topic>FUELS</topic><topic>LUBRICANTS</topic><topic>METALLURGY</topic><topic>PEAT</topic><topic>PETROLEUM, GAS OR COKE INDUSTRIES</topic><topic>TECHNICAL GASES CONTAINING CARBON MONOXIDE</topic><toplevel>online_resources</toplevel><creatorcontrib>YANAGAWA TOSHIO</creatorcontrib><creatorcontrib>FUKUDA TOMIYA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YANAGAWA TOSHIO</au><au>FUKUDA TOMIYA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PRODUCTION OF CHROME-CONTAINING COKE</title><date>1987-07-31</date><risdate>1987</risdate><abstract>PURPOSE:To obtain chrome-contg. coke with a reduced amt. of consumed coke, excellent heat economy and productivity, by blending a chrome ore in a powdery form and a particular reaction promoter with a raw material for production of coke and carbonizing the blend. CONSTITUTION:A raw material (A) for production of coke is blended with 45wt% or more chrome ore (B) in a powdery form from which coarse grains has been removed by sieving or pulverization and 0.1wt% or more at least one reaction promoter (C) selected from among an oxide, hydroxide, carbonate and borate of an alkali metal, an oxide, hydroxide and carbonate of boron and a fluoride of an alkaline earth metal to obtain a blend. Optionally, according to need, the blend is further blended with a binder such as PVA and molded into a shaped article. The blend or shaped article is put into a coke oven and heated at, e.g., 1,150-1,200 deg.C so as to effect reduction of the chrome component to a total conversion to metal of about 50%. Thus, the desired chrome-contg. coke is obtd.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPS62174291A
source esp@cenet
subjects CHEMISTRY
DESTRUCTIVE DISTILLATION OF CARBONAGEOUS MATERIALS FORPRODUCTION OF GAS, COKE, TAR, OR SIMILAR MATERIALS
FUELS
LUBRICANTS
METALLURGY
PEAT
PETROLEUM, GAS OR COKE INDUSTRIES
TECHNICAL GASES CONTAINING CARBON MONOXIDE
title PRODUCTION OF CHROME-CONTAINING COKE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-20T02%3A48%3A26IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YANAGAWA%20TOSHIO&rft.date=1987-07-31&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPS62174291A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true