METHOD FOR SUPPLYING PRELIMINARILY REDUCED ORE AT CONSTANT RATE TO MELT REDUCING DEVICE

PURPOSE:To maintain the constant rate characteristic in the amt. of the powder to be blown by detecting the layer thickness level of the powder flow in a powder supply outlet piping and controlling the supplying rate of a carrier gas in accordance with the signal thereof. CONSTITUTION:A thermocouple...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TAKEUCHI SHINOBU, IGAWA KATSUTOSHI, KATAYAMA EIJI, HAMADA HISAO, TAKADA SHIKO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator TAKEUCHI SHINOBU
IGAWA KATSUTOSHI
KATAYAMA EIJI
HAMADA HISAO
TAKADA SHIKO
description PURPOSE:To maintain the constant rate characteristic in the amt. of the powder to be blown by detecting the layer thickness level of the powder flow in a powder supply outlet piping and controlling the supplying rate of a carrier gas in accordance with the signal thereof. CONSTITUTION:A thermocouple 16 is installed in the outlet piping 7 of a device for supplying preliminarily sintered ore and the powder layer level in the piping 7 is continuously monitored. A regulating valve 19 is regulated via a transmission system 17 by an automatic control device 18 for the amt. of the carrier gas to decrease the amt. of the carrier gas when the temp. difference between the upper limit of the level at which the thermocouple 16 is inserted into the pipe and the target decreases to about 300-500 deg.C or below. The amt. of the carrier gas is increased when the above-mentioned temp. difference exceeds about 300-500 deg.C. The amt. of the powder to be blown is maintained constant by the above-mentioned method even if the temp. and density of the powder changes.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPS62133009A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPS62133009A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPS62133009A3</originalsourceid><addsrcrecordid>eNqNy00KwjAQQOFsXIh6h_EAQjUguAzJ1Ebyx2SqdFWKxJVood4fET2Aq7f53lxcPHITDdSRILcpuc6GIyRCZ70NiqzrgNC0Gg1EQlAMOobMKjCQYgSO4NHxF31eg2ercSlmt-E-ldWvC7GukXWzKeOzL9M4XMujvPpTyvvdVsqqOij5j3kD1a0xPQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR SUPPLYING PRELIMINARILY REDUCED ORE AT CONSTANT RATE TO MELT REDUCING DEVICE</title><source>esp@cenet</source><creator>TAKEUCHI SHINOBU ; IGAWA KATSUTOSHI ; KATAYAMA EIJI ; HAMADA HISAO ; TAKADA SHIKO</creator><creatorcontrib>TAKEUCHI SHINOBU ; IGAWA KATSUTOSHI ; KATAYAMA EIJI ; HAMADA HISAO ; TAKADA SHIKO</creatorcontrib><description>PURPOSE:To maintain the constant rate characteristic in the amt. of the powder to be blown by detecting the layer thickness level of the powder flow in a powder supply outlet piping and controlling the supplying rate of a carrier gas in accordance with the signal thereof. CONSTITUTION:A thermocouple 16 is installed in the outlet piping 7 of a device for supplying preliminarily sintered ore and the powder layer level in the piping 7 is continuously monitored. A regulating valve 19 is regulated via a transmission system 17 by an automatic control device 18 for the amt. of the carrier gas to decrease the amt. of the carrier gas when the temp. difference between the upper limit of the level at which the thermocouple 16 is inserted into the pipe and the target decreases to about 300-500 deg.C or below. The amt. of the carrier gas is increased when the above-mentioned temp. difference exceeds about 300-500 deg.C. The amt. of the powder to be blown is maintained constant by the above-mentioned method even if the temp. and density of the powder changes.</description><language>eng</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; MANUFACTURE OF IRON OR STEEL ; METALLURGY ; METALLURGY OF IRON ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>1987</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19870616&amp;DB=EPODOC&amp;CC=JP&amp;NR=S62133009A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19870616&amp;DB=EPODOC&amp;CC=JP&amp;NR=S62133009A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TAKEUCHI SHINOBU</creatorcontrib><creatorcontrib>IGAWA KATSUTOSHI</creatorcontrib><creatorcontrib>KATAYAMA EIJI</creatorcontrib><creatorcontrib>HAMADA HISAO</creatorcontrib><creatorcontrib>TAKADA SHIKO</creatorcontrib><title>METHOD FOR SUPPLYING PRELIMINARILY REDUCED ORE AT CONSTANT RATE TO MELT REDUCING DEVICE</title><description>PURPOSE:To maintain the constant rate characteristic in the amt. of the powder to be blown by detecting the layer thickness level of the powder flow in a powder supply outlet piping and controlling the supplying rate of a carrier gas in accordance with the signal thereof. CONSTITUTION:A thermocouple 16 is installed in the outlet piping 7 of a device for supplying preliminarily sintered ore and the powder layer level in the piping 7 is continuously monitored. A regulating valve 19 is regulated via a transmission system 17 by an automatic control device 18 for the amt. of the carrier gas to decrease the amt. of the carrier gas when the temp. difference between the upper limit of the level at which the thermocouple 16 is inserted into the pipe and the target decreases to about 300-500 deg.C or below. The amt. of the carrier gas is increased when the above-mentioned temp. difference exceeds about 300-500 deg.C. The amt. of the powder to be blown is maintained constant by the above-mentioned method even if the temp. and density of the powder changes.</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>MANUFACTURE OF IRON OR STEEL</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1987</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNy00KwjAQQOFsXIh6h_EAQjUguAzJ1Ebyx2SqdFWKxJVood4fET2Aq7f53lxcPHITDdSRILcpuc6GIyRCZ70NiqzrgNC0Gg1EQlAMOobMKjCQYgSO4NHxF31eg2ercSlmt-E-ldWvC7GukXWzKeOzL9M4XMujvPpTyvvdVsqqOij5j3kD1a0xPQ</recordid><startdate>19870616</startdate><enddate>19870616</enddate><creator>TAKEUCHI SHINOBU</creator><creator>IGAWA KATSUTOSHI</creator><creator>KATAYAMA EIJI</creator><creator>HAMADA HISAO</creator><creator>TAKADA SHIKO</creator><scope>EVB</scope></search><sort><creationdate>19870616</creationdate><title>METHOD FOR SUPPLYING PRELIMINARILY REDUCED ORE AT CONSTANT RATE TO MELT REDUCING DEVICE</title><author>TAKEUCHI SHINOBU ; IGAWA KATSUTOSHI ; KATAYAMA EIJI ; HAMADA HISAO ; TAKADA SHIKO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPS62133009A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1987</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>MANUFACTURE OF IRON OR STEEL</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>TAKEUCHI SHINOBU</creatorcontrib><creatorcontrib>IGAWA KATSUTOSHI</creatorcontrib><creatorcontrib>KATAYAMA EIJI</creatorcontrib><creatorcontrib>HAMADA HISAO</creatorcontrib><creatorcontrib>TAKADA SHIKO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TAKEUCHI SHINOBU</au><au>IGAWA KATSUTOSHI</au><au>KATAYAMA EIJI</au><au>HAMADA HISAO</au><au>TAKADA SHIKO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR SUPPLYING PRELIMINARILY REDUCED ORE AT CONSTANT RATE TO MELT REDUCING DEVICE</title><date>1987-06-16</date><risdate>1987</risdate><abstract>PURPOSE:To maintain the constant rate characteristic in the amt. of the powder to be blown by detecting the layer thickness level of the powder flow in a powder supply outlet piping and controlling the supplying rate of a carrier gas in accordance with the signal thereof. CONSTITUTION:A thermocouple 16 is installed in the outlet piping 7 of a device for supplying preliminarily sintered ore and the powder layer level in the piping 7 is continuously monitored. A regulating valve 19 is regulated via a transmission system 17 by an automatic control device 18 for the amt. of the carrier gas to decrease the amt. of the carrier gas when the temp. difference between the upper limit of the level at which the thermocouple 16 is inserted into the pipe and the target decreases to about 300-500 deg.C or below. The amt. of the carrier gas is increased when the above-mentioned temp. difference exceeds about 300-500 deg.C. The amt. of the powder to be blown is maintained constant by the above-mentioned method even if the temp. and density of the powder changes.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPS62133009A
source esp@cenet
subjects CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
MANUFACTURE OF IRON OR STEEL
METALLURGY
METALLURGY OF IRON
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title METHOD FOR SUPPLYING PRELIMINARILY REDUCED ORE AT CONSTANT RATE TO MELT REDUCING DEVICE
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-07T13%3A43%3A49IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TAKEUCHI%20SHINOBU&rft.date=1987-06-16&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPS62133009A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true