MANUFACTURE OF MARAGING STEEL
PURPOSE:To improve the yield and workability by carrying out electroslag remelting using a CaF2-Al2O3-TiO2 flux contg. C and Si restricted to prescribed amounts. CONSTITUTION:Molten metal melted in a primary melting furnace is charged into a VOD furnace. While agitating the molten metal by blowing A...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PURPOSE:To improve the yield and workability by carrying out electroslag remelting using a CaF2-Al2O3-TiO2 flux contg. C and Si restricted to prescribed amounts. CONSTITUTION:Molten metal melted in a primary melting furnace is charged into a VOD furnace. While agitating the molten metal by blowing Ar, O2 is blown to decarburize and desiliconize the molten metal, and the resulting steel material is used as an electrode. A CaF2-Al2O3-TiO2 or CaF2-CaO-Al2O3-TiO2 flux contg. |
---|