DIRECT SPIN-DRAW PROCESS FOR HIGH-DURABILITY NYLON-6 YARN

PURPOSE:A nylon 6 of a specific relative viscosity is spun into an undrawn yarn of low crystallinity and high optical birefringence, subsequently subjected to heat drawing under specific conditions to produce the titled yarn which is suitable for use in rubber reinforcement, because of its high dime...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: KIRIYAMA SHIYUNICHI, SUGIE TSUTOMU, YOKOYAMA HIROSHI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator KIRIYAMA SHIYUNICHI
SUGIE TSUTOMU
YOKOYAMA HIROSHI
description PURPOSE:A nylon 6 of a specific relative viscosity is spun into an undrawn yarn of low crystallinity and high optical birefringence, subsequently subjected to heat drawing under specific conditions to produce the titled yarn which is suitable for use in rubber reinforcement, because of its high dimensional stability and high economic efficiency. CONSTITUTION:A nylon 6 of 3.1-4.0 relative viscosity is made into a yarn at a speed of less than 2,000m/min to form an undrawn yarn of lower crystallinity and (20-45)X10 optical birefringence (DELTAn), then the undrawn yarn is subjected to 2 or less staged thermal drawing so that DELTAn becomes 55-62X10, and wound up at a speed of lower than 4,000m/min to produce a nylon 6 of high durability. The undrawn yarn is preferably solidified under conditions of pX1 in DELTAn=ASP (A is constant; S is spinning speed) and the solidification is effected by the horizontal air blowing and front face sucking method.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPS59144608A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPS59144608A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPS59144608A3</originalsourceid><addsrcrecordid>eNrjZLB08QxydQ5RCA7w9NN1CXIMVwgI8nd2DQ5WcPMPUvDwdPfQdQkNcnTy9PEMiVTwi_Tx99M1U4h0DPLjYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxXgHBppaGJiZmBhaOxsSoAQCO3SkL</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>DIRECT SPIN-DRAW PROCESS FOR HIGH-DURABILITY NYLON-6 YARN</title><source>esp@cenet</source><creator>KIRIYAMA SHIYUNICHI ; SUGIE TSUTOMU ; YOKOYAMA HIROSHI</creator><creatorcontrib>KIRIYAMA SHIYUNICHI ; SUGIE TSUTOMU ; YOKOYAMA HIROSHI</creatorcontrib><description>PURPOSE:A nylon 6 of a specific relative viscosity is spun into an undrawn yarn of low crystallinity and high optical birefringence, subsequently subjected to heat drawing under specific conditions to produce the titled yarn which is suitable for use in rubber reinforcement, because of its high dimensional stability and high economic efficiency. CONSTITUTION:A nylon 6 of 3.1-4.0 relative viscosity is made into a yarn at a speed of less than 2,000m/min to form an undrawn yarn of lower crystallinity and (20-45)X10&lt;-3&gt; optical birefringence (DELTAn), then the undrawn yarn is subjected to 2 or less staged thermal drawing so that DELTAn becomes 55-62X10&lt;-3&gt;, and wound up at a speed of lower than 4,000m/min to produce a nylon 6 of high durability. The undrawn yarn is preferably solidified under conditions of pX1 in DELTAn=ASP (A is constant; S is spinning speed) and the solidification is effected by the horizontal air blowing and front face sucking method.</description><language>eng</language><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS ; CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS ; NATURAL OR ARTIFICIAL THREADS OR FIBRES ; SPINNING ; TEXTILES</subject><creationdate>1984</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19840818&amp;DB=EPODOC&amp;CC=JP&amp;NR=S59144608A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19840818&amp;DB=EPODOC&amp;CC=JP&amp;NR=S59144608A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>KIRIYAMA SHIYUNICHI</creatorcontrib><creatorcontrib>SUGIE TSUTOMU</creatorcontrib><creatorcontrib>YOKOYAMA HIROSHI</creatorcontrib><title>DIRECT SPIN-DRAW PROCESS FOR HIGH-DURABILITY NYLON-6 YARN</title><description>PURPOSE:A nylon 6 of a specific relative viscosity is spun into an undrawn yarn of low crystallinity and high optical birefringence, subsequently subjected to heat drawing under specific conditions to produce the titled yarn which is suitable for use in rubber reinforcement, because of its high dimensional stability and high economic efficiency. CONSTITUTION:A nylon 6 of 3.1-4.0 relative viscosity is made into a yarn at a speed of less than 2,000m/min to form an undrawn yarn of lower crystallinity and (20-45)X10&lt;-3&gt; optical birefringence (DELTAn), then the undrawn yarn is subjected to 2 or less staged thermal drawing so that DELTAn becomes 55-62X10&lt;-3&gt;, and wound up at a speed of lower than 4,000m/min to produce a nylon 6 of high durability. The undrawn yarn is preferably solidified under conditions of pX1 in DELTAn=ASP (A is constant; S is spinning speed) and the solidification is effected by the horizontal air blowing and front face sucking method.</description><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</subject><subject>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</subject><subject>NATURAL OR ARTIFICIAL THREADS OR FIBRES</subject><subject>SPINNING</subject><subject>TEXTILES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1984</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLB08QxydQ5RCA7w9NN1CXIMVwgI8nd2DQ5WcPMPUvDwdPfQdQkNcnTy9PEMiVTwi_Tx99M1U4h0DPLjYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxXgHBppaGJiZmBhaOxsSoAQCO3SkL</recordid><startdate>19840818</startdate><enddate>19840818</enddate><creator>KIRIYAMA SHIYUNICHI</creator><creator>SUGIE TSUTOMU</creator><creator>YOKOYAMA HIROSHI</creator><scope>EVB</scope></search><sort><creationdate>19840818</creationdate><title>DIRECT SPIN-DRAW PROCESS FOR HIGH-DURABILITY NYLON-6 YARN</title><author>KIRIYAMA SHIYUNICHI ; SUGIE TSUTOMU ; YOKOYAMA HIROSHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPS59144608A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1984</creationdate><topic>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</topic><topic>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</topic><topic>NATURAL OR ARTIFICIAL THREADS OR FIBRES</topic><topic>SPINNING</topic><topic>TEXTILES</topic><toplevel>online_resources</toplevel><creatorcontrib>KIRIYAMA SHIYUNICHI</creatorcontrib><creatorcontrib>SUGIE TSUTOMU</creatorcontrib><creatorcontrib>YOKOYAMA HIROSHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>KIRIYAMA SHIYUNICHI</au><au>SUGIE TSUTOMU</au><au>YOKOYAMA HIROSHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>DIRECT SPIN-DRAW PROCESS FOR HIGH-DURABILITY NYLON-6 YARN</title><date>1984-08-18</date><risdate>1984</risdate><abstract>PURPOSE:A nylon 6 of a specific relative viscosity is spun into an undrawn yarn of low crystallinity and high optical birefringence, subsequently subjected to heat drawing under specific conditions to produce the titled yarn which is suitable for use in rubber reinforcement, because of its high dimensional stability and high economic efficiency. CONSTITUTION:A nylon 6 of 3.1-4.0 relative viscosity is made into a yarn at a speed of less than 2,000m/min to form an undrawn yarn of lower crystallinity and (20-45)X10&lt;-3&gt; optical birefringence (DELTAn), then the undrawn yarn is subjected to 2 or less staged thermal drawing so that DELTAn becomes 55-62X10&lt;-3&gt;, and wound up at a speed of lower than 4,000m/min to produce a nylon 6 of high durability. The undrawn yarn is preferably solidified under conditions of pX1 in DELTAn=ASP (A is constant; S is spinning speed) and the solidification is effected by the horizontal air blowing and front face sucking method.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPS59144608A
source esp@cenet
subjects APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS
CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS
NATURAL OR ARTIFICIAL THREADS OR FIBRES
SPINNING
TEXTILES
title DIRECT SPIN-DRAW PROCESS FOR HIGH-DURABILITY NYLON-6 YARN
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-05T01%3A39%3A00IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=KIRIYAMA%20SHIYUNICHI&rft.date=1984-08-18&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPS59144608A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true