METHOD FOR PREVENTING DEWING OF ANNEALED STEEL STRIP COIL

PURPOSE:To reduce the use of dehumidifying air for preventing dewing as far as possible by continuously measuring the bottom edge temp. of steel strip coils of a coil cooling shop, and blowing rust-inhibitive air thereto only when said temp. lowers below the specific temp. difference with respect to...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MIKI TETSUO, KIKUCHI MITSUTOSHI, OOKOUCHI TOSHIHIRO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MIKI TETSUO
KIKUCHI MITSUTOSHI
OOKOUCHI TOSHIHIRO
description PURPOSE:To reduce the use of dehumidifying air for preventing dewing as far as possible by continuously measuring the bottom edge temp. of steel strip coils of a coil cooling shop, and blowing rust-inhibitive air thereto only when said temp. lowers below the specific temp. difference with respect to room temp. CONSTITUTION:After annealed coils 22 are stacked on a coil base 21 in a coil cooling shop, cooling air is fed from an opening 23 to the central part of the coils, whereby the coils are cooled. After they are cooled down to prescribed temps., a damper 24 is commanded by a cylinder control valve 28 from a coil cooling controller to close the port 23, and this completes the cooling of the coils 22. The coils 22 are stored on the cooling base 21. During storage, the edge temp. of the coils 22 is continuously measured with a thermometer 27, and when it lowers =+3 deg.C.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPS5747834A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPS5747834A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPS5747834A3</originalsourceid><addsrcrecordid>eNrjZLD0dQ3x8HdRcPMPUggIcg1z9Qvx9HNXcHENB1H-bgqOfn6ujj6uLgrBIa6uPkAyyDNAwdnf04eHgTUtMac4lRdKczMouLmGOHvophbkx6cWFyQmp-allsR7BQSbmpuYWxibOBoToQQANSwojQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>METHOD FOR PREVENTING DEWING OF ANNEALED STEEL STRIP COIL</title><source>esp@cenet</source><creator>MIKI TETSUO ; KIKUCHI MITSUTOSHI ; OOKOUCHI TOSHIHIRO</creator><creatorcontrib>MIKI TETSUO ; KIKUCHI MITSUTOSHI ; OOKOUCHI TOSHIHIRO</creatorcontrib><description>PURPOSE:To reduce the use of dehumidifying air for preventing dewing as far as possible by continuously measuring the bottom edge temp. of steel strip coils of a coil cooling shop, and blowing rust-inhibitive air thereto only when said temp. lowers below the specific temp. difference with respect to room temp. CONSTITUTION:After annealed coils 22 are stacked on a coil base 21 in a coil cooling shop, cooling air is fed from an opening 23 to the central part of the coils, whereby the coils are cooled. After they are cooled down to prescribed temps., a damper 24 is commanded by a cylinder control valve 28 from a coil cooling controller to close the port 23, and this completes the cooling of the coils 22. The coils 22 are stored on the cooling base 21. During storage, the edge temp. of the coils 22 is continuously measured with a thermometer 27, and when it lowers &lt;=+3 deg.C with respect to room temp., dehumidifying air is blown to the center of the coils 22 through the opening 23 from a supply conduit 26 by opening a shutoff valve 30 by the command from a coil dewing alarm device, whereby dewing is prevented. The blowing is stopped when the temp. rises &gt;=+3 deg.C.</description><language>eng</language><subject>CHEMISTRY ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><creationdate>1982</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19820318&amp;DB=EPODOC&amp;CC=JP&amp;NR=S5747834A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19820318&amp;DB=EPODOC&amp;CC=JP&amp;NR=S5747834A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MIKI TETSUO</creatorcontrib><creatorcontrib>KIKUCHI MITSUTOSHI</creatorcontrib><creatorcontrib>OOKOUCHI TOSHIHIRO</creatorcontrib><title>METHOD FOR PREVENTING DEWING OF ANNEALED STEEL STRIP COIL</title><description>PURPOSE:To reduce the use of dehumidifying air for preventing dewing as far as possible by continuously measuring the bottom edge temp. of steel strip coils of a coil cooling shop, and blowing rust-inhibitive air thereto only when said temp. lowers below the specific temp. difference with respect to room temp. CONSTITUTION:After annealed coils 22 are stacked on a coil base 21 in a coil cooling shop, cooling air is fed from an opening 23 to the central part of the coils, whereby the coils are cooled. After they are cooled down to prescribed temps., a damper 24 is commanded by a cylinder control valve 28 from a coil cooling controller to close the port 23, and this completes the cooling of the coils 22. The coils 22 are stored on the cooling base 21. During storage, the edge temp. of the coils 22 is continuously measured with a thermometer 27, and when it lowers &lt;=+3 deg.C with respect to room temp., dehumidifying air is blown to the center of the coils 22 through the opening 23 from a supply conduit 26 by opening a shutoff valve 30 by the command from a coil dewing alarm device, whereby dewing is prevented. The blowing is stopped when the temp. rises &gt;=+3 deg.C.</description><subject>CHEMISTRY</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1982</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLD0dQ3x8HdRcPMPUggIcg1z9Qvx9HNXcHENB1H-bgqOfn6ujj6uLgrBIa6uPkAyyDNAwdnf04eHgTUtMac4lRdKczMouLmGOHvophbkx6cWFyQmp-allsR7BQSbmpuYWxibOBoToQQANSwojQ</recordid><startdate>19820318</startdate><enddate>19820318</enddate><creator>MIKI TETSUO</creator><creator>KIKUCHI MITSUTOSHI</creator><creator>OOKOUCHI TOSHIHIRO</creator><scope>EVB</scope></search><sort><creationdate>19820318</creationdate><title>METHOD FOR PREVENTING DEWING OF ANNEALED STEEL STRIP COIL</title><author>MIKI TETSUO ; KIKUCHI MITSUTOSHI ; OOKOUCHI TOSHIHIRO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPS5747834A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1982</creationdate><topic>CHEMISTRY</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>MIKI TETSUO</creatorcontrib><creatorcontrib>KIKUCHI MITSUTOSHI</creatorcontrib><creatorcontrib>OOKOUCHI TOSHIHIRO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MIKI TETSUO</au><au>KIKUCHI MITSUTOSHI</au><au>OOKOUCHI TOSHIHIRO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>METHOD FOR PREVENTING DEWING OF ANNEALED STEEL STRIP COIL</title><date>1982-03-18</date><risdate>1982</risdate><abstract>PURPOSE:To reduce the use of dehumidifying air for preventing dewing as far as possible by continuously measuring the bottom edge temp. of steel strip coils of a coil cooling shop, and blowing rust-inhibitive air thereto only when said temp. lowers below the specific temp. difference with respect to room temp. CONSTITUTION:After annealed coils 22 are stacked on a coil base 21 in a coil cooling shop, cooling air is fed from an opening 23 to the central part of the coils, whereby the coils are cooled. After they are cooled down to prescribed temps., a damper 24 is commanded by a cylinder control valve 28 from a coil cooling controller to close the port 23, and this completes the cooling of the coils 22. The coils 22 are stored on the cooling base 21. During storage, the edge temp. of the coils 22 is continuously measured with a thermometer 27, and when it lowers &lt;=+3 deg.C with respect to room temp., dehumidifying air is blown to the center of the coils 22 through the opening 23 from a supply conduit 26 by opening a shutoff valve 30 by the command from a coil dewing alarm device, whereby dewing is prevented. The blowing is stopped when the temp. rises &gt;=+3 deg.C.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPS5747834A
source esp@cenet
subjects CHEMISTRY
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
title METHOD FOR PREVENTING DEWING OF ANNEALED STEEL STRIP COIL
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-03T20%3A04%3A15IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MIKI%20TETSUO&rft.date=1982-03-18&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPS5747834A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true