CALCINED POWDER FOR PRODUCING BI-CONTAINING OXIDE SUPERCONDUCTOR AND BI-2223 PHASE POLYCRYSTALLINE BODY OBTAINED BY SINTERING SAME
PROBLEM TO BE SOLVED: To stably obtain a superconductor having high Jc by preparing calcined powder having a specified average particle diameter blended so as to give the compsn. of Bi-2223 phase crystals and sintering the powder contg. Bi-2212 phase crystals, impurity phases and a specified amt. or...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To stably obtain a superconductor having high Jc by preparing calcined powder having a specified average particle diameter blended so as to give the compsn. of Bi-2223 phase crystals and sintering the powder contg. Bi-2212 phase crystals, impurity phases and a specified amt. or less of carbon. SOLUTION: This polycrystalline body obtd. by sintering the calcined powder has >=9,000A/cm Jc. The Bi-2223 phase crystals are represented by the formula Bia -Pbb -Src -Cad -Cu3 -Ox (where 1.20 |
---|