APATITE SLURRY AND ITS PRODUCTION
PROBLEM TO BE SOLVED: To provide an apatite slurry by substantially completely redispersing secondary particles of apatite, and to provide its production method. SOLUTION: This apatite slurry is produced by dispersing apatite particles in an org. solvent having solubility with water. This slurry sho...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To provide an apatite slurry by substantially completely redispersing secondary particles of apatite, and to provide its production method. SOLUTION: This apatite slurry is produced by dispersing apatite particles in an org. solvent having solubility with water. This slurry shows such a dispersion state that the average particle size of the apatite particles is =3μm particle size are substantially not present. The apatite slurry is obtd. by dispersing apatite particles in an org. solvent having solubility with water, supplying the slurry to a stirring mill to pulverize and disperse to such a dispersion degree that particles having >=3μm particle size are substantially not present. |
---|