ANTICORROSIVE STEEL PIPE
PROBLEM TO BE SOLVED: To simultaneously prevent oxygen corrosion of an inner surface generated by flowing of water (non-deairing) at an ambient temperature and sulfuric acid corrosion of an outer surface generated by adhesion of sulfuric acid to the outer surface due to dewing, in the case of attain...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PROBLEM TO BE SOLVED: To simultaneously prevent oxygen corrosion of an inner surface generated by flowing of water (non-deairing) at an ambient temperature and sulfuric acid corrosion of an outer surface generated by adhesion of sulfuric acid to the outer surface due to dewing, in the case of attaining increase of a recovery heat from exhaust gas in an economizer of a boiler. SOLUTION: An economizer 10 is constituted of an anticorrosive steel pipe formed in a double pipe structure which comprises an inner surface side formed of a stainless steel pipe 1 and an outer surface side formed of a sulfuric acid dew point corrosive resistant steel pipe 2. |
---|