PREPARATION OF FIBER MAT AND MOLDED ITEM AND PRESS MOLDED ITEM

PURPOSE: To produce a formed article at a low energy cost and having light weight by press forming a fiber mat comprising a mixed material of a high melting point matrix and low melting point bonding component while preheating only a plane area to be formed. CONSTITUTION: Fiber mat is formed by usin...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TOOMASU YOOSUTO, GERUHARUTO MIYURAA-BURORU, RAINHARUTO SHIYUTEIIFU
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator TOOMASU YOOSUTO
GERUHARUTO MIYURAA-BURORU
RAINHARUTO SHIYUTEIIFU
description PURPOSE: To produce a formed article at a low energy cost and having light weight by press forming a fiber mat comprising a mixed material of a high melting point matrix and low melting point bonding component while preheating only a plane area to be formed. CONSTITUTION: Fiber mat is formed by using polyester having a denier of 1-200 dTex and a fiber length of 5 mm or endless, polyamide, cotton, celulosic and/or viscose fibers as the high melting matrix and polyester or polyamide having a similar denier and fiber length as described above whose melting point is at least 10 deg.C or lower as the bonding component as the bonding component and by uniformly blending the above high melting matrix with the above bonding component in the blend ratio of 10-40% by weight. And, after preheating only a plane area of the mat to be formed between an electric heating plate of the same size and an opposite plate, under hot wind conducting condition at a temp. of 40-80 deg.C higher than the melting point of the above combining bonding for 30-180 seconds, the formed mat is continuously press-formed to the fixed form at a temp. of 30-80 deg.C lower than the melting point of the prescribed bonding component for 30-180 seconds.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPH06184902A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPH06184902A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPH06184902A3</originalsourceid><addsrcrecordid>eNrjZLALCHINcAxyDPH091Pwd1Nw83RyDVLwdQxRcPRzUfD193FxdVHwDHH1BfOBioODkUV5GFjTEnOKU3mhNDeDoptriLOHbmpBfnxqcUFicmpeakm8V4CHgZmhhYmlgZGjMTFqABz-KcI</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>PREPARATION OF FIBER MAT AND MOLDED ITEM AND PRESS MOLDED ITEM</title><source>esp@cenet</source><creator>TOOMASU YOOSUTO ; GERUHARUTO MIYURAA-BURORU ; RAINHARUTO SHIYUTEIIFU</creator><creatorcontrib>TOOMASU YOOSUTO ; GERUHARUTO MIYURAA-BURORU ; RAINHARUTO SHIYUTEIIFU</creatorcontrib><description>PURPOSE: To produce a formed article at a low energy cost and having light weight by press forming a fiber mat comprising a mixed material of a high melting point matrix and low melting point bonding component while preheating only a plane area to be formed. CONSTITUTION: Fiber mat is formed by using polyester having a denier of 1-200 dTex and a fiber length of 5 mm or endless, polyamide, cotton, celulosic and/or viscose fibers as the high melting matrix and polyester or polyamide having a similar denier and fiber length as described above whose melting point is at least 10 deg.C or lower as the bonding component as the bonding component and by uniformly blending the above high melting matrix with the above bonding component in the blend ratio of 10-40% by weight. And, after preheating only a plane area of the mat to be formed between an electric heating plate of the same size and an opposite plate, under hot wind conducting condition at a temp. of 40-80 deg.C higher than the melting point of the above combining bonding for 30-180 seconds, the formed mat is continuously press-formed to the fixed form at a temp. of 30-80 deg.C lower than the melting point of the prescribed bonding component for 30-180 seconds.</description><edition>5</edition><language>eng</language><subject>BRAIDING ; COTTON-WOOL ; FABRICS MADE BY SUCH PROCESSES OR APPARATUS, e.g. FELTS,NON-WOVEN FABRICS ; KNITTING ; LACE-MAKING ; MAKING TEXTILE FABRICS, e.g. FROM FIBRES OR FILAMENTARYMATERIAL ; NON-WOVEN FABRICS ; PERFORMING OPERATIONS ; TEXTILES ; TRANSPORTING ; TRIMMINGS ; VEHICLES IN GENERAL ; VEHICLES, VEHICLE FITTINGS, OR VEHICLE PARTS, NOT OTHERWISEPROVIDED FOR ; WADDING</subject><creationdate>1994</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19940705&amp;DB=EPODOC&amp;CC=JP&amp;NR=H06184902A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19940705&amp;DB=EPODOC&amp;CC=JP&amp;NR=H06184902A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>TOOMASU YOOSUTO</creatorcontrib><creatorcontrib>GERUHARUTO MIYURAA-BURORU</creatorcontrib><creatorcontrib>RAINHARUTO SHIYUTEIIFU</creatorcontrib><title>PREPARATION OF FIBER MAT AND MOLDED ITEM AND PRESS MOLDED ITEM</title><description>PURPOSE: To produce a formed article at a low energy cost and having light weight by press forming a fiber mat comprising a mixed material of a high melting point matrix and low melting point bonding component while preheating only a plane area to be formed. CONSTITUTION: Fiber mat is formed by using polyester having a denier of 1-200 dTex and a fiber length of 5 mm or endless, polyamide, cotton, celulosic and/or viscose fibers as the high melting matrix and polyester or polyamide having a similar denier and fiber length as described above whose melting point is at least 10 deg.C or lower as the bonding component as the bonding component and by uniformly blending the above high melting matrix with the above bonding component in the blend ratio of 10-40% by weight. And, after preheating only a plane area of the mat to be formed between an electric heating plate of the same size and an opposite plate, under hot wind conducting condition at a temp. of 40-80 deg.C higher than the melting point of the above combining bonding for 30-180 seconds, the formed mat is continuously press-formed to the fixed form at a temp. of 30-80 deg.C lower than the melting point of the prescribed bonding component for 30-180 seconds.</description><subject>BRAIDING</subject><subject>COTTON-WOOL</subject><subject>FABRICS MADE BY SUCH PROCESSES OR APPARATUS, e.g. FELTS,NON-WOVEN FABRICS</subject><subject>KNITTING</subject><subject>LACE-MAKING</subject><subject>MAKING TEXTILE FABRICS, e.g. FROM FIBRES OR FILAMENTARYMATERIAL</subject><subject>NON-WOVEN FABRICS</subject><subject>PERFORMING OPERATIONS</subject><subject>TEXTILES</subject><subject>TRANSPORTING</subject><subject>TRIMMINGS</subject><subject>VEHICLES IN GENERAL</subject><subject>VEHICLES, VEHICLE FITTINGS, OR VEHICLE PARTS, NOT OTHERWISEPROVIDED FOR</subject><subject>WADDING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1994</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLALCHINcAxyDPH091Pwd1Nw83RyDVLwdQxRcPRzUfD193FxdVHwDHH1BfOBioODkUV5GFjTEnOKU3mhNDeDoptriLOHbmpBfnxqcUFicmpeakm8V4CHgZmhhYmlgZGjMTFqABz-KcI</recordid><startdate>19940705</startdate><enddate>19940705</enddate><creator>TOOMASU YOOSUTO</creator><creator>GERUHARUTO MIYURAA-BURORU</creator><creator>RAINHARUTO SHIYUTEIIFU</creator><scope>EVB</scope></search><sort><creationdate>19940705</creationdate><title>PREPARATION OF FIBER MAT AND MOLDED ITEM AND PRESS MOLDED ITEM</title><author>TOOMASU YOOSUTO ; GERUHARUTO MIYURAA-BURORU ; RAINHARUTO SHIYUTEIIFU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPH06184902A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1994</creationdate><topic>BRAIDING</topic><topic>COTTON-WOOL</topic><topic>FABRICS MADE BY SUCH PROCESSES OR APPARATUS, e.g. FELTS,NON-WOVEN FABRICS</topic><topic>KNITTING</topic><topic>LACE-MAKING</topic><topic>MAKING TEXTILE FABRICS, e.g. FROM FIBRES OR FILAMENTARYMATERIAL</topic><topic>NON-WOVEN FABRICS</topic><topic>PERFORMING OPERATIONS</topic><topic>TEXTILES</topic><topic>TRANSPORTING</topic><topic>TRIMMINGS</topic><topic>VEHICLES IN GENERAL</topic><topic>VEHICLES, VEHICLE FITTINGS, OR VEHICLE PARTS, NOT OTHERWISEPROVIDED FOR</topic><topic>WADDING</topic><toplevel>online_resources</toplevel><creatorcontrib>TOOMASU YOOSUTO</creatorcontrib><creatorcontrib>GERUHARUTO MIYURAA-BURORU</creatorcontrib><creatorcontrib>RAINHARUTO SHIYUTEIIFU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>TOOMASU YOOSUTO</au><au>GERUHARUTO MIYURAA-BURORU</au><au>RAINHARUTO SHIYUTEIIFU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>PREPARATION OF FIBER MAT AND MOLDED ITEM AND PRESS MOLDED ITEM</title><date>1994-07-05</date><risdate>1994</risdate><abstract>PURPOSE: To produce a formed article at a low energy cost and having light weight by press forming a fiber mat comprising a mixed material of a high melting point matrix and low melting point bonding component while preheating only a plane area to be formed. CONSTITUTION: Fiber mat is formed by using polyester having a denier of 1-200 dTex and a fiber length of 5 mm or endless, polyamide, cotton, celulosic and/or viscose fibers as the high melting matrix and polyester or polyamide having a similar denier and fiber length as described above whose melting point is at least 10 deg.C or lower as the bonding component as the bonding component and by uniformly blending the above high melting matrix with the above bonding component in the blend ratio of 10-40% by weight. And, after preheating only a plane area of the mat to be formed between an electric heating plate of the same size and an opposite plate, under hot wind conducting condition at a temp. of 40-80 deg.C higher than the melting point of the above combining bonding for 30-180 seconds, the formed mat is continuously press-formed to the fixed form at a temp. of 30-80 deg.C lower than the melting point of the prescribed bonding component for 30-180 seconds.</abstract><edition>5</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPH06184902A
source esp@cenet
subjects BRAIDING
COTTON-WOOL
FABRICS MADE BY SUCH PROCESSES OR APPARATUS, e.g. FELTS,NON-WOVEN FABRICS
KNITTING
LACE-MAKING
MAKING TEXTILE FABRICS, e.g. FROM FIBRES OR FILAMENTARYMATERIAL
NON-WOVEN FABRICS
PERFORMING OPERATIONS
TEXTILES
TRANSPORTING
TRIMMINGS
VEHICLES IN GENERAL
VEHICLES, VEHICLE FITTINGS, OR VEHICLE PARTS, NOT OTHERWISEPROVIDED FOR
WADDING
title PREPARATION OF FIBER MAT AND MOLDED ITEM AND PRESS MOLDED ITEM
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-11T07%3A07%3A20IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=TOOMASU%20YOOSUTO&rft.date=1994-07-05&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPH06184902A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true