BRICK FOR MOLTEN IRON PRETREATMENT VESSEL

PURPOSE:To improve the oxidation resistnacs, slag resistance, spalling resistance and low heat conductivity by incorporating anthracter coal containing the sepecifc quantity of fixed carbon and volatile matter as an aggregate. CONSTITUTION:The anthracite coal which is >=90wt.% fixed carbon, =1.62...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MATSUMOTO YOSHIO, KURAYOSHI KAZUMI, NAKAGAWA HITOSHI, NAGAISHI NAOHITO, KAWASAKI KAZUHIKO, YOSHITOMI TAKENORI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MATSUMOTO YOSHIO
KURAYOSHI KAZUMI
NAKAGAWA HITOSHI
NAGAISHI NAOHITO
KAWASAKI KAZUHIKO
YOSHITOMI TAKENORI
description PURPOSE:To improve the oxidation resistnacs, slag resistance, spalling resistance and low heat conductivity by incorporating anthracter coal containing the sepecifc quantity of fixed carbon and volatile matter as an aggregate. CONSTITUTION:The anthracite coal which is >=90wt.% fixed carbon, =1.62 the apparent sepcific gravity and >=1mm the particle size is obtained by selecting from a carbon source as the aggregate. Then, 3-20wt.% anthacite coal, the alumina souce of an electrode alumina, etc., incorporating >=50wt.% Al2O3 as necessary, and the binder of a phonol resin, etc., for SiC Mg, etc., are kneaded and molded to obtain a molded product. Then, the molded product is subjected to a heat treatment, etc., at the temp.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPH061650A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPH061650A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPH061650A3</originalsourceid><addsrcrecordid>eNrjZNB0CvJ09lZw8w9S8PX3CXH1U_AM8vdTCAhyDQlydQzxdfULUQhzDQ529eFhYE1LzClO5YXS3Azybq4hzh66qQX58anFBYnJqXmpJfFeAR4GZoZmpgaOxoRVAACuAyPY</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>BRICK FOR MOLTEN IRON PRETREATMENT VESSEL</title><source>esp@cenet</source><creator>MATSUMOTO YOSHIO ; KURAYOSHI KAZUMI ; NAKAGAWA HITOSHI ; NAGAISHI NAOHITO ; KAWASAKI KAZUHIKO ; YOSHITOMI TAKENORI</creator><creatorcontrib>MATSUMOTO YOSHIO ; KURAYOSHI KAZUMI ; NAKAGAWA HITOSHI ; NAGAISHI NAOHITO ; KAWASAKI KAZUHIKO ; YOSHITOMI TAKENORI</creatorcontrib><description>PURPOSE:To improve the oxidation resistnacs, slag resistance, spalling resistance and low heat conductivity by incorporating anthracter coal containing the sepecifc quantity of fixed carbon and volatile matter as an aggregate. CONSTITUTION:The anthracite coal which is &gt;=90wt.% fixed carbon, &lt;=3wt.% a volatile matter, &gt;=1.62 the apparent sepcific gravity and &gt;=1mm the particle size is obtained by selecting from a carbon source as the aggregate. Then, 3-20wt.% anthacite coal, the alumina souce of an electrode alumina, etc., incorporating &gt;=50wt.% Al2O3 as necessary, and the binder of a phonol resin, etc., for SiC Mg, etc., are kneaded and molded to obtain a molded product. Then, the molded product is subjected to a heat treatment, etc., at the temp. &lt;=300 deg.C, to produce the brick for molten iron preteatment vessel.</description><edition>5</edition><language>eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>1994</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19940111&amp;DB=EPODOC&amp;CC=JP&amp;NR=H061650A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19940111&amp;DB=EPODOC&amp;CC=JP&amp;NR=H061650A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MATSUMOTO YOSHIO</creatorcontrib><creatorcontrib>KURAYOSHI KAZUMI</creatorcontrib><creatorcontrib>NAKAGAWA HITOSHI</creatorcontrib><creatorcontrib>NAGAISHI NAOHITO</creatorcontrib><creatorcontrib>KAWASAKI KAZUHIKO</creatorcontrib><creatorcontrib>YOSHITOMI TAKENORI</creatorcontrib><title>BRICK FOR MOLTEN IRON PRETREATMENT VESSEL</title><description>PURPOSE:To improve the oxidation resistnacs, slag resistance, spalling resistance and low heat conductivity by incorporating anthracter coal containing the sepecifc quantity of fixed carbon and volatile matter as an aggregate. CONSTITUTION:The anthracite coal which is &gt;=90wt.% fixed carbon, &lt;=3wt.% a volatile matter, &gt;=1.62 the apparent sepcific gravity and &gt;=1mm the particle size is obtained by selecting from a carbon source as the aggregate. Then, 3-20wt.% anthacite coal, the alumina souce of an electrode alumina, etc., incorporating &gt;=50wt.% Al2O3 as necessary, and the binder of a phonol resin, etc., for SiC Mg, etc., are kneaded and molded to obtain a molded product. Then, the molded product is subjected to a heat treatment, etc., at the temp. &lt;=300 deg.C, to produce the brick for molten iron preteatment vessel.</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1994</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNB0CvJ09lZw8w9S8PX3CXH1U_AM8vdTCAhyDQlydQzxdfULUQhzDQ529eFhYE1LzClO5YXS3Azybq4hzh66qQX58anFBYnJqXmpJfFeAR4GZoZmpgaOxoRVAACuAyPY</recordid><startdate>19940111</startdate><enddate>19940111</enddate><creator>MATSUMOTO YOSHIO</creator><creator>KURAYOSHI KAZUMI</creator><creator>NAKAGAWA HITOSHI</creator><creator>NAGAISHI NAOHITO</creator><creator>KAWASAKI KAZUHIKO</creator><creator>YOSHITOMI TAKENORI</creator><scope>EVB</scope></search><sort><creationdate>19940111</creationdate><title>BRICK FOR MOLTEN IRON PRETREATMENT VESSEL</title><author>MATSUMOTO YOSHIO ; KURAYOSHI KAZUMI ; NAKAGAWA HITOSHI ; NAGAISHI NAOHITO ; KAWASAKI KAZUHIKO ; YOSHITOMI TAKENORI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPH061650A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1994</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>MATSUMOTO YOSHIO</creatorcontrib><creatorcontrib>KURAYOSHI KAZUMI</creatorcontrib><creatorcontrib>NAKAGAWA HITOSHI</creatorcontrib><creatorcontrib>NAGAISHI NAOHITO</creatorcontrib><creatorcontrib>KAWASAKI KAZUHIKO</creatorcontrib><creatorcontrib>YOSHITOMI TAKENORI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MATSUMOTO YOSHIO</au><au>KURAYOSHI KAZUMI</au><au>NAKAGAWA HITOSHI</au><au>NAGAISHI NAOHITO</au><au>KAWASAKI KAZUHIKO</au><au>YOSHITOMI TAKENORI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>BRICK FOR MOLTEN IRON PRETREATMENT VESSEL</title><date>1994-01-11</date><risdate>1994</risdate><abstract>PURPOSE:To improve the oxidation resistnacs, slag resistance, spalling resistance and low heat conductivity by incorporating anthracter coal containing the sepecifc quantity of fixed carbon and volatile matter as an aggregate. CONSTITUTION:The anthracite coal which is &gt;=90wt.% fixed carbon, &lt;=3wt.% a volatile matter, &gt;=1.62 the apparent sepcific gravity and &gt;=1mm the particle size is obtained by selecting from a carbon source as the aggregate. Then, 3-20wt.% anthacite coal, the alumina souce of an electrode alumina, etc., incorporating &gt;=50wt.% Al2O3 as necessary, and the binder of a phonol resin, etc., for SiC Mg, etc., are kneaded and molded to obtain a molded product. Then, the molded product is subjected to a heat treatment, etc., at the temp. &lt;=300 deg.C, to produce the brick for molten iron preteatment vessel.</abstract><edition>5</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPH061650A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title BRICK FOR MOLTEN IRON PRETREATMENT VESSEL
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-26T03%3A24%3A06IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MATSUMOTO%20YOSHIO&rft.date=1994-01-11&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPH061650A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true