BRICK FOR MOLTEN IRON PRETREATMENT VESSEL

PURPOSE:To improve the oxidation resistnacs, slag resistance, spalling resistance and low heat conductivity by incorporating anthracter coal containing the sepecifc quantity of fixed carbon and volatile matter as an aggregate. CONSTITUTION:The anthracite coal which is >=90wt.% fixed carbon, =1.62...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MATSUMOTO YOSHIO, KURAYOSHI KAZUMI, NAKAGAWA HITOSHI, NAGAISHI NAOHITO, KAWASAKI KAZUHIKO, YOSHITOMI TAKENORI
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:PURPOSE:To improve the oxidation resistnacs, slag resistance, spalling resistance and low heat conductivity by incorporating anthracter coal containing the sepecifc quantity of fixed carbon and volatile matter as an aggregate. CONSTITUTION:The anthracite coal which is >=90wt.% fixed carbon, =1.62 the apparent sepcific gravity and >=1mm the particle size is obtained by selecting from a carbon source as the aggregate. Then, 3-20wt.% anthacite coal, the alumina souce of an electrode alumina, etc., incorporating >=50wt.% Al2O3 as necessary, and the binder of a phonol resin, etc., for SiC Mg, etc., are kneaded and molded to obtain a molded product. Then, the molded product is subjected to a heat treatment, etc., at the temp.