JPH05307961

PURPOSE:To prevent the condition that the gas is generated at the time of contact of a current collecting bar, which is inserted into a gel-like negative electrode, with zinc by iron, nickel, chrome and metal oxide adhering or biting to the surface of the current collecting bar during the processing...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ITO YUKIHIRO, OTOMO EIJI, YONEYAMA KUNIO, IIZUKA KAZUO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ITO YUKIHIRO
OTOMO EIJI
YONEYAMA KUNIO
IIZUKA KAZUO
description PURPOSE:To prevent the condition that the gas is generated at the time of contact of a current collecting bar, which is inserted into a gel-like negative electrode, with zinc by iron, nickel, chrome and metal oxide adhering or biting to the surface of the current collecting bar during the processing and that the internal pressure of the battery rises to operate a safety valve and hinder the use of the battery. CONSTITUTION:A current collecting bar 8 is inserted into a gel-like negative electrode 4, which includes zinc and alkaline electrolyte, to form an alkaline dry battery. The current collecting bar 8 made of brass is processed into a linear shape by hot extrusion, and thereafter, mechanical skin peeling at 0.01mm or more of thickness is performed. The skin peeling can be performed by mechanical polishing.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JPH05307961A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JPH05307961A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JPH05307961A3</originalsourceid><addsrcrecordid>eNrjZOD2CvAwMDU2MLc0M-RhYE1LzClO5YXS3AyKbq4hzh66qQX58anFBYnJqXmpJfFIOhyNiVEDAD8UG7M</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>JPH05307961</title><source>esp@cenet</source><creator>ITO YUKIHIRO ; OTOMO EIJI ; YONEYAMA KUNIO ; IIZUKA KAZUO</creator><creatorcontrib>ITO YUKIHIRO ; OTOMO EIJI ; YONEYAMA KUNIO ; IIZUKA KAZUO</creatorcontrib><description>PURPOSE:To prevent the condition that the gas is generated at the time of contact of a current collecting bar, which is inserted into a gel-like negative electrode, with zinc by iron, nickel, chrome and metal oxide adhering or biting to the surface of the current collecting bar during the processing and that the internal pressure of the battery rises to operate a safety valve and hinder the use of the battery. CONSTITUTION:A current collecting bar 8 is inserted into a gel-like negative electrode 4, which includes zinc and alkaline electrolyte, to form an alkaline dry battery. The current collecting bar 8 made of brass is processed into a linear shape by hot extrusion, and thereafter, mechanical skin peeling at 0.01mm or more of thickness is performed. The skin peeling can be performed by mechanical polishing.</description><edition>5</edition><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; ELECTRICITY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>1993</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19931119&amp;DB=EPODOC&amp;CC=JP&amp;NR=H05307961A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19931119&amp;DB=EPODOC&amp;CC=JP&amp;NR=H05307961A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ITO YUKIHIRO</creatorcontrib><creatorcontrib>OTOMO EIJI</creatorcontrib><creatorcontrib>YONEYAMA KUNIO</creatorcontrib><creatorcontrib>IIZUKA KAZUO</creatorcontrib><title>JPH05307961</title><description>PURPOSE:To prevent the condition that the gas is generated at the time of contact of a current collecting bar, which is inserted into a gel-like negative electrode, with zinc by iron, nickel, chrome and metal oxide adhering or biting to the surface of the current collecting bar during the processing and that the internal pressure of the battery rises to operate a safety valve and hinder the use of the battery. CONSTITUTION:A current collecting bar 8 is inserted into a gel-like negative electrode 4, which includes zinc and alkaline electrolyte, to form an alkaline dry battery. The current collecting bar 8 made of brass is processed into a linear shape by hot extrusion, and thereafter, mechanical skin peeling at 0.01mm or more of thickness is performed. The skin peeling can be performed by mechanical polishing.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>ELECTRICITY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1993</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZOD2CvAwMDU2MLc0M-RhYE1LzClO5YXS3AyKbq4hzh66qQX58anFBYnJqXmpJfFIOhyNiVEDAD8UG7M</recordid><startdate>19931119</startdate><enddate>19931119</enddate><creator>ITO YUKIHIRO</creator><creator>OTOMO EIJI</creator><creator>YONEYAMA KUNIO</creator><creator>IIZUKA KAZUO</creator><scope>EVB</scope></search><sort><creationdate>19931119</creationdate><title>JPH05307961</title><author>ITO YUKIHIRO ; OTOMO EIJI ; YONEYAMA KUNIO ; IIZUKA KAZUO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JPH05307961A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>1993</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>ELECTRICITY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>ITO YUKIHIRO</creatorcontrib><creatorcontrib>OTOMO EIJI</creatorcontrib><creatorcontrib>YONEYAMA KUNIO</creatorcontrib><creatorcontrib>IIZUKA KAZUO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ITO YUKIHIRO</au><au>OTOMO EIJI</au><au>YONEYAMA KUNIO</au><au>IIZUKA KAZUO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>JPH05307961</title><date>1993-11-19</date><risdate>1993</risdate><abstract>PURPOSE:To prevent the condition that the gas is generated at the time of contact of a current collecting bar, which is inserted into a gel-like negative electrode, with zinc by iron, nickel, chrome and metal oxide adhering or biting to the surface of the current collecting bar during the processing and that the internal pressure of the battery rises to operate a safety valve and hinder the use of the battery. CONSTITUTION:A current collecting bar 8 is inserted into a gel-like negative electrode 4, which includes zinc and alkaline electrolyte, to form an alkaline dry battery. The current collecting bar 8 made of brass is processed into a linear shape by hot extrusion, and thereafter, mechanical skin peeling at 0.01mm or more of thickness is performed. The skin peeling can be performed by mechanical polishing.</abstract><edition>5</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_JPH05307961A
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
ELECTRICITY
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
title JPH05307961
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-07T11%3A08%3A28IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ITO%20YUKIHIRO&rft.date=1993-11-19&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJPH05307961A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true