JPH0248613B
PURPOSE:To give excellent creep rupture strength at high temp. required to for atomic reactor, etc., by limiting composition of ferrite steel and making it tempered martensite structure containing delta-ferrite phase or tempered martensite single phase structure by heat-treatment. CONSTITUTION:The f...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | PURPOSE:To give excellent creep rupture strength at high temp. required to for atomic reactor, etc., by limiting composition of ferrite steel and making it tempered martensite structure containing delta-ferrite phase or tempered martensite single phase structure by heat-treatment. CONSTITUTION:The ferrite steel is composed of by wt% of 0.02-0.15% C, |
---|