Beschreibung
Zusammenfassung:A fire resistance barrier comprises a glass fiber fabric coated with not less than 3% by weight of an organic polymer which on pyrolysis (15 min at 600.degree.C) leaves not less than 20% of a carbon-con-taining residue.