JP2790714B

The present invention provides microwave ceramic dielectric materials having large relative dielectric constant, very large Q, and stable and small temperature coefficient. The ceramic dielectric materials of the present invention are expressed by the general formula: [{BaO}x{TiO2}y{(Sm2O3)1-m-n(SrO...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WATAI HISAO, SAITO KYOSHI, PPONDA TOSHIHISA, UCHIUMI YOSHIKAZU, YAMADA RO
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The present invention provides microwave ceramic dielectric materials having large relative dielectric constant, very large Q, and stable and small temperature coefficient. The ceramic dielectric materials of the present invention are expressed by the general formula: [{BaO}x{TiO2}y{(Sm2O3)1-m-n(SrO.CeO2)m(CaO.CeO2)n}z]1-A[SrTiO3]A wherein, 0.1