Ferromagnetic metal particles of substantially iron are prepared by starting from an acicular alpha -FeOOH, applying a shape-stabilizing finish to the particle surface, heating at 500 DEG -850 DEG C. and subsequently reducing with gaseous reducing agents at 200 DEG -500 DEG C. to the metal, and star...
Gespeichert in:
Hauptverfasser: | , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Ferromagnetic metal particles of substantially iron are prepared by starting from an acicular alpha -FeOOH, applying a shape-stabilizing finish to the particle surface, heating at 500 DEG -850 DEG C. and subsequently reducing with gaseous reducing agents at 200 DEG -500 DEG C. to the metal, and starting alpha -FeOOH being prepared in the presence of zinc and phosphate ions. |
---|