METHOD FOR CARBONATING AND CURING PRECAST CONCRETE MEMBER
To provide a simple method for carbonating and curing a precast concrete member, which does not require large-scale construction or modification of a facility itself, and does not require occupancy of the entire facility until the end of carbonation curing.SOLUTION: A method of the present invention...
Gespeichert in:
Hauptverfasser: | , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To provide a simple method for carbonating and curing a precast concrete member, which does not require large-scale construction or modification of a facility itself, and does not require occupancy of the entire facility until the end of carbonation curing.SOLUTION: A method of the present invention for carbonating and curing a precast concrete member includes: a precast concrete producing step of casting a fresh concrete into a formwork and curing the same to obtain one or more precast concrete members having a porosity of 5% or more and 45% or less; a drying step of drying the precast concrete members until the unit water content of the precast concrete members is reduced to 5.0% or more; and a carbonating-and-curing step of carbonating and curing the precast concrete member after drying, which is loaded on a pallet and enclosed by an enclosure member, by supplying a carbon dioxide-containing gas to the inside of the enclosure member.SELECTED DRAWING: Figure 1
【課題】施設自体の大規模な築造や改造が不要であると共に、炭酸化養生終了までの施設全体の占有が不要である、簡便なプレキャストコンクリート部材の炭酸化養生方法を提供する。【解決手段】本発明のプレキャストコンクリート部材の炭酸化養生方法は、フレッシュコンクリートを型枠に打設して硬化させて、5%以上45%以下の空隙率を有する1つ以上のプレキャストコンクリート部材を得るプレキャストコンクリート生成工程と、前記プレキャストコンクリート部材の単位水量の減少率が5.0%以上になるまで、前記プレキャストコンクリート部材を乾燥させる乾燥工程と、パレット上に積載され、囲み部材で囲まれている乾燥後のプレキャストコンクリート部材を、前記囲み部材の内部に炭酸ガス含有ガスを供給して、炭酸化養生する、炭酸化養生工程と、を有する。【選択図】図1 |
---|