POLYETHYLENE-BASED THERMAL DECOMPOSITION WAX AND PRODUCTION METHOD THEREOF
To provide polyethylene-based thermal decomposition wax which shows little fuming during high-temperature processing and little stickiness of a molded body comprising the wax, has excellent blocking resistance, and is of low cost.SOLUTION: Provided is polyethylene-based thermal decomposition wax whi...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To provide polyethylene-based thermal decomposition wax which shows little fuming during high-temperature processing and little stickiness of a molded body comprising the wax, has excellent blocking resistance, and is of low cost.SOLUTION: Provided is polyethylene-based thermal decomposition wax which satisfies the following requirements (1) to (3): (1) a percentage content of a compound having a molecular weight of 500 or less, as determined by gel permeation chromatography (GPC), is 1.5 wt.% or less; (2) a number average molecular weight (Mn), as measured by GPC, is 500 to 10,000; and (3) a ratio of a number average molecular weight (Mn) and a weight average molecular eight (Mw), Mw/Mn, as measured by GPC, is 3.5 or less.SELECTED DRAWING: None
【課題】 高温加工時の発煙やワックスを含有する成形体のべたつきが少なく、耐ブロッキング性に優れ、かつ低コストであるポリエチレン系熱分解ワックスを提供する。【解決手段】 下記(1)~(3)の要件を満足する、ポリエチレン系熱分解ワックス。(1)ゲル・パーミエーション・クロマトグラフィー(GPC)によって得られた分子量500以下の化合物の含有率が1.5重量%以下である。(2)GPCによって測定した数平均分子量(Mn)が500以上10,000以下である。(3)GPCによって測定した数平均分子量(Mn)と重量平均分子量(Mw)の比:Mw/Mnの値が3.5以下である。【選択図】 なし |
---|