LAMINATE AND PACKAGING BAG

To provide a laminate which is suitable as a packaging material that enables packaging of an article used in a clean environment, and is excellent in recyclability.SOLUTION: A laminate includes at least a first resin layer and a second resin layer, wherein the first resin layer is provided so as to...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TAKASUGI YUYA, KASHIWABARA TOMOMI
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To provide a laminate which is suitable as a packaging material that enables packaging of an article used in a clean environment, and is excellent in recyclability.SOLUTION: A laminate includes at least a first resin layer and a second resin layer, wherein the first resin layer is provided so as to be peeled from the second resin layer, peeling strength between the first resin layer and the second resin layer, which is measured under the conditions of peeling angle of 180 degrees and test speed of 50 mm/min, is 1.0 N/15 mm width or less, the second resin layer is a sealant layer containing polyolefin as a main component, and a content ratio of the polyolefin in the second resin layer is 82 mass% or more based on the mass of the second resin layer.SELECTED DRAWING: Figure 1 【課題】クリーン環境内で使用される物品を包装できる包装材料として好適で、リサイクル性に優れる積層体を提供する。【解決手段】第1の樹脂層と、第2の樹脂層と、を少なくとも備える積層体であって、第1の樹脂層は、第2の樹脂層から剥離できるように設けられており、剥離角度:180度、試験速度:50mm/minの条件にて測定される、第1の樹脂層と第2の樹脂層との剥離強度は、1.0N/15mm幅以下であり、第2の樹脂層は、ポリオレフィンを主成分として含有するシーラント層であり、第2の樹脂層におけるポリオレフィンの含有割合は、第2の樹脂層の質量を基準として、82質量%以上である、積層体。【選択図】図1