RESIN FILM AND LAMINATE TUBE CONTAINER
To provide a laminate tube container with a resin film capable of improving environmental load reduction and capable of improving slipperiness and toughness.SOLUTION: A laminate tube container of the present invention includes: a head portion including a shoulder portion and a spout portion; and a b...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To provide a laminate tube container with a resin film capable of improving environmental load reduction and capable of improving slipperiness and toughness.SOLUTION: A laminate tube container of the present invention includes: a head portion including a shoulder portion and a spout portion; and a body portion connected to the shoulder portion of the head portion, where the body portion is composed of a laminate including at least an outer sealant layer, a base material layer. and an inner sealant layer in this order. The inner sealant layer includes a resin film including at least a first layer and a second layer, where the first layer constitutes at least one outermost layer of the resin film, the first layer and the second layer are directly laminated, the first layer is made of a fossil fuel-derived polyethylene resin, the second layer is made of a resin containing a biomass-derived linear low density resin, the density of the second layer is lower than the density of the first layer, the difference in density between the second layer and the first layer is 0.003 g/cm3 or more, and the stiffness parameter (K) of the resin film defined by a specific formula is 3.5 or more and 6.5 or less.SELECTED DRAWING: Figure 1
【課題】環境負荷低減性を向上させることができると共に、滑り性及び剛性を向上させることができる樹脂フィルムを備えるラミネートチューブ容器の提供。【解決手段】本発明のラミネートチューブ容器は、肩部及び注出口部からなる頭部と、前記頭部の前記肩部と連結した胴部と、を備え、前記胴部が、外側シーラント層と、基材層と、内側シーラント層とを少なくとも順に備える積層体から構成され、前記内側シーラント層が、第1層と、第2層とを少なくとも備える樹脂フィルムを備え、第1層が、樹脂フィルムの少なくとも一方の最外層を構成し、第1層と、前記第2層とが、直接積層され、第1層が、化石燃料由来のポリエチレン樹脂から構成され、第2層が、バイオマス由来の直鎖状低密度ポリエチレンを含む樹脂により構成され、第2層の密度が、第1層の密度よりも小さく、前記第2層と、前記第1層との密度差が、0.003g/cm3以上であり、特定の式により規定される樹脂フィルムの剛性パラメータ(K)が、3.5以上6.5以下である。【選択図】図1 |
---|