HEAT-FUSIBLE LAMINATE FILM
To provide a polyolefin-based laminate film containing polypropylene and having reduced environmental loads by using a biomass-derived resin, which has improved film formation property.SOLUTION: A laminate film has (A) a seal layer, (B) a core layer and (C) a laminate layer, where (A) the seal layer...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To provide a polyolefin-based laminate film containing polypropylene and having reduced environmental loads by using a biomass-derived resin, which has improved film formation property.SOLUTION: A laminate film has (A) a seal layer, (B) a core layer and (C) a laminate layer, where (A) the seal layer and (C) the laminate layer contain polypropylene, (B) the core layer contains linear low-density polyethylene and biomass-derived low density polyethylene, and crystal heat of fusion ΔH observed in a temperature range of 90-110°C in a second heating process of a DSC curve is 4.8 to 23.2 J/g.SELECTED DRAWING: None
【課題】ポリプロピレンを含有するポリオレフィン系の積層フィルムであって、バイオマス由来の樹脂を使用することにより環境負荷が低減された積層フィルムにおいて、更に製膜性等が向上した積層フィルムを提供する。【解決手段】(A)シール層、(B)コア層、及び(C)ラミネート層を有する積層フィルムであって、(A)シール層、及び(C)ラミネート層がポリプロピレンを含有し、(B)コア層が直鎖状低密度ポリエチレン及びバイオマス由来の低密度ポリエチレンを含有し、DSC曲線の第2回昇温行程の90から110℃の温度範囲で観測される結晶融解熱量ΔHが4.8~23.2J/gである、上記積層フィルム。【選択図】 なし |
---|