COLD APPLICATION-TYPE ASPHALT MIXTURE AND MANUFACTURING METHOD THEREFOR
To provide a cold application-type asphalt mixture which has excellent storage stability and with which high initial strength after construction can be achieved.SOLUTION: A cold application-type asphalt mixture 7 includes: aggregates 1; a binder layer 2 containing asphalt and fatty acid and covering...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | OGURA TAKUMI MIYAJI MASAHIRO NAGASAKI HIROSHI |
description | To provide a cold application-type asphalt mixture which has excellent storage stability and with which high initial strength after construction can be achieved.SOLUTION: A cold application-type asphalt mixture 7 includes: aggregates 1; a binder layer 2 containing asphalt and fatty acid and covering the periphery of the aggregates 1; an alkaline additive layer 3 covering the periphery of the binder layer 2; and a condensed hydroxy fatty acid layer 4 covering the periphery of the alkaline additive layer 3. Since an outer surface of the cold application-type asphalt mixture 7 is coated with the condensed hydroxy fatty acid layer 4, the reaction with moisture in the air is suppressed and the storage stability is improved. And by increasing the amount of the alkaline additive added to the cold application-type asphalt mixture 7, the hardening reaction during construction is accelerated, and the initial strength after construction increases.SELECTED DRAWING: Figure 1
【課題】優れた貯蔵安定性を有し、施工後に高い初期強度を実現できる常温アスファルト合材を提供する。【解決手段】常温施工型アスファルト合材7は、骨材1と、アスファルト及び脂肪酸を含み骨材1の周囲を覆うバインダ層2と、バインダ層2の周囲を覆うアルカリ性添加材層3と、アルカリ性添加材層3の周囲を覆う縮合ヒドロキシ脂肪酸層4とを備える。常温施工型アスファルト合材7の外面は、縮合ヒドロキシ脂肪酸層4によって被覆されているため、空気中の水分との反応が抑制され、貯蔵安定性が高くなる。また、常温施工型アスファルト合材7に添加するアルカリ性添加材の量を増やすことで施工時における硬化反応を早め、施工後の初期強度が高くなる。【選択図】図1 |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_JP2023097822A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>JP2023097822A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_JP2023097822A3</originalsourceid><addsrcrecordid>eNrjZHB39vdxUXAMCPDxdHYM8fT30w2JDHBVcAwO8HD0CVHw9YwICQ0C8v1cFHwd_ULdHJ2BfE8_dwVf1xAPfxeFEA_XIFc3_yAeBta0xJziVF4ozc2g5OYa4uyhm1qQH59aXJCYnJqXWhLvFWBkYGRsYGluYWTkaEyUIgBR_C1P</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>COLD APPLICATION-TYPE ASPHALT MIXTURE AND MANUFACTURING METHOD THEREFOR</title><source>esp@cenet</source><creator>OGURA TAKUMI ; MIYAJI MASAHIRO ; NAGASAKI HIROSHI</creator><creatorcontrib>OGURA TAKUMI ; MIYAJI MASAHIRO ; NAGASAKI HIROSHI</creatorcontrib><description>To provide a cold application-type asphalt mixture which has excellent storage stability and with which high initial strength after construction can be achieved.SOLUTION: A cold application-type asphalt mixture 7 includes: aggregates 1; a binder layer 2 containing asphalt and fatty acid and covering the periphery of the aggregates 1; an alkaline additive layer 3 covering the periphery of the binder layer 2; and a condensed hydroxy fatty acid layer 4 covering the periphery of the alkaline additive layer 3. Since an outer surface of the cold application-type asphalt mixture 7 is coated with the condensed hydroxy fatty acid layer 4, the reaction with moisture in the air is suppressed and the storage stability is improved. And by increasing the amount of the alkaline additive added to the cold application-type asphalt mixture 7, the hardening reaction during construction is accelerated, and the initial strength after construction increases.SELECTED DRAWING: Figure 1
【課題】優れた貯蔵安定性を有し、施工後に高い初期強度を実現できる常温アスファルト合材を提供する。【解決手段】常温施工型アスファルト合材7は、骨材1と、アスファルト及び脂肪酸を含み骨材1の周囲を覆うバインダ層2と、バインダ層2の周囲を覆うアルカリ性添加材層3と、アルカリ性添加材層3の周囲を覆う縮合ヒドロキシ脂肪酸層4とを備える。常温施工型アスファルト合材7の外面は、縮合ヒドロキシ脂肪酸層4によって被覆されているため、空気中の水分との反応が抑制され、貯蔵安定性が高くなる。また、常温施工型アスファルト合材7に添加するアルカリ性添加材の量を増やすことで施工時における硬化反応を早め、施工後の初期強度が高くなる。【選択図】図1</description><language>eng ; jpn</language><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; CONSTRUCTION OF ROADS, RAILWAYS, OR BRIDGES ; CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, ORTHE LIKE ; FIXED CONSTRUCTIONS ; GENERAL PROCESSES OF COMPOUNDING ; MACHINES OR AUXILIARY TOOLS FOR CONSTRUCTION OR REPAIR ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; WORKING-UP</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230710&DB=EPODOC&CC=JP&NR=2023097822A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20230710&DB=EPODOC&CC=JP&NR=2023097822A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>OGURA TAKUMI</creatorcontrib><creatorcontrib>MIYAJI MASAHIRO</creatorcontrib><creatorcontrib>NAGASAKI HIROSHI</creatorcontrib><title>COLD APPLICATION-TYPE ASPHALT MIXTURE AND MANUFACTURING METHOD THEREFOR</title><description>To provide a cold application-type asphalt mixture which has excellent storage stability and with which high initial strength after construction can be achieved.SOLUTION: A cold application-type asphalt mixture 7 includes: aggregates 1; a binder layer 2 containing asphalt and fatty acid and covering the periphery of the aggregates 1; an alkaline additive layer 3 covering the periphery of the binder layer 2; and a condensed hydroxy fatty acid layer 4 covering the periphery of the alkaline additive layer 3. Since an outer surface of the cold application-type asphalt mixture 7 is coated with the condensed hydroxy fatty acid layer 4, the reaction with moisture in the air is suppressed and the storage stability is improved. And by increasing the amount of the alkaline additive added to the cold application-type asphalt mixture 7, the hardening reaction during construction is accelerated, and the initial strength after construction increases.SELECTED DRAWING: Figure 1
【課題】優れた貯蔵安定性を有し、施工後に高い初期強度を実現できる常温アスファルト合材を提供する。【解決手段】常温施工型アスファルト合材7は、骨材1と、アスファルト及び脂肪酸を含み骨材1の周囲を覆うバインダ層2と、バインダ層2の周囲を覆うアルカリ性添加材層3と、アルカリ性添加材層3の周囲を覆う縮合ヒドロキシ脂肪酸層4とを備える。常温施工型アスファルト合材7の外面は、縮合ヒドロキシ脂肪酸層4によって被覆されているため、空気中の水分との反応が抑制され、貯蔵安定性が高くなる。また、常温施工型アスファルト合材7に添加するアルカリ性添加材の量を増やすことで施工時における硬化反応を早め、施工後の初期強度が高くなる。【選択図】図1</description><subject>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>CONSTRUCTION OF ROADS, RAILWAYS, OR BRIDGES</subject><subject>CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, ORTHE LIKE</subject><subject>FIXED CONSTRUCTIONS</subject><subject>GENERAL PROCESSES OF COMPOUNDING</subject><subject>MACHINES OR AUXILIARY TOOLS FOR CONSTRUCTION OR REPAIR</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>WORKING-UP</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHB39vdxUXAMCPDxdHYM8fT30w2JDHBVcAwO8HD0CVHw9YwICQ0C8v1cFHwd_ULdHJ2BfE8_dwVf1xAPfxeFEA_XIFc3_yAeBta0xJziVF4ozc2g5OYa4uyhm1qQH59aXJCYnJqXWhLvFWBkYGRsYGluYWTkaEyUIgBR_C1P</recordid><startdate>20230710</startdate><enddate>20230710</enddate><creator>OGURA TAKUMI</creator><creator>MIYAJI MASAHIRO</creator><creator>NAGASAKI HIROSHI</creator><scope>EVB</scope></search><sort><creationdate>20230710</creationdate><title>COLD APPLICATION-TYPE ASPHALT MIXTURE AND MANUFACTURING METHOD THEREFOR</title><author>OGURA TAKUMI ; MIYAJI MASAHIRO ; NAGASAKI HIROSHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_JP2023097822A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; jpn</language><creationdate>2023</creationdate><topic>AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>CONSTRUCTION OF ROADS, RAILWAYS, OR BRIDGES</topic><topic>CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, ORTHE LIKE</topic><topic>FIXED CONSTRUCTIONS</topic><topic>GENERAL PROCESSES OF COMPOUNDING</topic><topic>MACHINES OR AUXILIARY TOOLS FOR CONSTRUCTION OR REPAIR</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>WORKING-UP</topic><toplevel>online_resources</toplevel><creatorcontrib>OGURA TAKUMI</creatorcontrib><creatorcontrib>MIYAJI MASAHIRO</creatorcontrib><creatorcontrib>NAGASAKI HIROSHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>OGURA TAKUMI</au><au>MIYAJI MASAHIRO</au><au>NAGASAKI HIROSHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>COLD APPLICATION-TYPE ASPHALT MIXTURE AND MANUFACTURING METHOD THEREFOR</title><date>2023-07-10</date><risdate>2023</risdate><abstract>To provide a cold application-type asphalt mixture which has excellent storage stability and with which high initial strength after construction can be achieved.SOLUTION: A cold application-type asphalt mixture 7 includes: aggregates 1; a binder layer 2 containing asphalt and fatty acid and covering the periphery of the aggregates 1; an alkaline additive layer 3 covering the periphery of the binder layer 2; and a condensed hydroxy fatty acid layer 4 covering the periphery of the alkaline additive layer 3. Since an outer surface of the cold application-type asphalt mixture 7 is coated with the condensed hydroxy fatty acid layer 4, the reaction with moisture in the air is suppressed and the storage stability is improved. And by increasing the amount of the alkaline additive added to the cold application-type asphalt mixture 7, the hardening reaction during construction is accelerated, and the initial strength after construction increases.SELECTED DRAWING: Figure 1
【課題】優れた貯蔵安定性を有し、施工後に高い初期強度を実現できる常温アスファルト合材を提供する。【解決手段】常温施工型アスファルト合材7は、骨材1と、アスファルト及び脂肪酸を含み骨材1の周囲を覆うバインダ層2と、バインダ層2の周囲を覆うアルカリ性添加材層3と、アルカリ性添加材層3の周囲を覆う縮合ヒドロキシ脂肪酸層4とを備える。常温施工型アスファルト合材7の外面は、縮合ヒドロキシ脂肪酸層4によって被覆されているため、空気中の水分との反応が抑制され、貯蔵安定性が高くなる。また、常温施工型アスファルト合材7に添加するアルカリ性添加材の量を増やすことで施工時における硬化反応を早め、施工後の初期強度が高くなる。【選択図】図1</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | eng ; jpn |
recordid | cdi_epo_espacenet_JP2023097822A |
source | esp@cenet |
subjects | AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F,C08G CHEMISTRY COMPOSITIONS BASED THEREON CONSTRUCTION OF ROADS, RAILWAYS, OR BRIDGES CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, ORTHE LIKE FIXED CONSTRUCTIONS GENERAL PROCESSES OF COMPOUNDING MACHINES OR AUXILIARY TOOLS FOR CONSTRUCTION OR REPAIR METALLURGY ORGANIC MACROMOLECULAR COMPOUNDS THEIR PREPARATION OR CHEMICAL WORKING-UP WORKING-UP |
title | COLD APPLICATION-TYPE ASPHALT MIXTURE AND MANUFACTURING METHOD THEREFOR |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-18T04%3A47%3A19IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=OGURA%20TAKUMI&rft.date=2023-07-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EJP2023097822A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |