MODIFIED CELLULOSE AND RESIN COMPOSITION
To provide a modified cellulose fiber formed from a biodegradable component and useful as a reinforcing material for resin.SOLUTION: A modified cellulose is prepared by modifying a cellulose fiber with 3-hydroxybutyric acid or an oligomer thereof. In the modified cellulose, the 3-hydroxybutyric acid...
Gespeichert in:
Hauptverfasser: | , , , , , |
---|---|
Format: | Patent |
Sprache: | eng ; jpn |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To provide a modified cellulose fiber formed from a biodegradable component and useful as a reinforcing material for resin.SOLUTION: A modified cellulose is prepared by modifying a cellulose fiber with 3-hydroxybutyric acid or an oligomer thereof. In the modified cellulose, the 3-hydroxybutyric acid or oligomer thereof may be ester-bonded to the 6-position of the anhydroglucose unit of the cellulose fiber. The 3-hydroxybutyric acid or oligomer thereof may have an average degree of polymerization of 1 to 10. The grafting rate of the 3-hydroxybutyric acid or oligomer thereof may be 5 to 30 mol%. The 3-hydroxybutyric acid may be R-3-hydroxybutyric acid.SELECTED DRAWING: None
【課題】生分解性成分で形成され、樹脂に対する補強材として有用な変性セルロース繊維を提供する。【解決手段】セルロース繊維に、3-ヒドロキシ酪酸またはそのオリゴマーが変性した変性セルロースを調製する。前記変性セルロースは、前記セルロース繊維の無水グルコース単位の6位に、前記3-ヒドロキシ酪酸またはそのオリゴマーがエステル結合していてもよい。前記3-ヒドロキシ酪酸またはそのオリゴマーの平均重合度は1~10であってもよい。前記3-ヒドロキシ酪酸またはそのオリゴマーによるグラフト化率は5~30モル%であってもよい。前記3-ヒドロキシ酪酸はR-3-ヒドロキシ酪酸であってもよい。【選択図】なし |
---|