STEEL FOR DIE-CASTING MOLD

To provide a steel for a die-casting mold that retains high toughness even when the hardness after tempering is increased.SOLUTION: A steel for a die-casting mold contains, in mass%, 0.35≤C≤0.41, 0.05≤Si≤0.15, 0.70≤Mn≤1.00, 5.60≤Cr≤6.10, 2.40≤Mo≤2.60, 0.60≤V≤0.70, Ni≤0.25, Cu≤0.25, Al≤0.030, N≤0.025...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: TENG HUI LIN, TATSUYA MASAKATSU, HIGUCHI SHIGEKI, HASUNO AKIHITO
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To provide a steel for a die-casting mold that retains high toughness even when the hardness after tempering is increased.SOLUTION: A steel for a die-casting mold contains, in mass%, 0.35≤C≤0.41, 0.05≤Si≤0.15, 0.70≤Mn≤1.00, 5.60≤Cr≤6.10, 2.40≤Mo≤2.60, 0.60≤V≤0.70, Ni≤0.25, Cu≤0.25, Al≤0.030, N≤0.0250, O≤0.0030, P≤0.030 with the balance being Fe and inevitable impurities.SELECTED DRAWING: None 【課題】調質後の硬さを高めた場合でも高靭性を維持することができるダイカスト金型用鋼を提供する。【解決手段】ダイカスト金型用の鋼は、質量%で0.35≦C≦0.41、0.05≦Si≦0.15、0.70≦Mn≦1.00、5.60≦Cr≦6.10、2.40≦Mo≦2.60、0.60≦V≦0.70、Ni≦0.25、Cu≦0.25、Al≦0.030、N≦0.0250、O≦0.0030、P≦0.030を含有し、残部がFe及び不可避的不純物の組成を有する。【選択図】 なし