SODIUM FERRITE PARTICLE POWDER AND METHOD FOR PRODUCING THE SAME

To provide a sodium ferrite particle powder that adsorbs carbon dioxide in the temperature range from room temperature to 100°C, can recover carbon dioxide by heating at 150°C or less, and have excellent moldability and processability, and to provide a method for producing the particle powder.SOLUTI...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SHIMO SHINYA, SAKAMOTO MUNEYOSHI, KURITA EIICHI
Format: Patent
Sprache:eng ; jpn
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:To provide a sodium ferrite particle powder that adsorbs carbon dioxide in the temperature range from room temperature to 100°C, can recover carbon dioxide by heating at 150°C or less, and have excellent moldability and processability, and to provide a method for producing the particle powder.SOLUTION: Provided is a sodium ferrite particle powder in which, characterized, at least one or more metals selected from the group of trivalent metals consisting of Al, Ga, In, Cr, Mn, Co, Rh, Sc, Y and Ce exist in a solid solution state or in a state having no specific crystal forms by 0.05 to 5 wt.% in terms of oxide, and the mole ratio of Na/Fe is 0.75 to 1.25.SELECTED DRAWING: None 【課題】本発明は、二酸化炭素を室温から100℃までの温度範囲で吸着し、150℃以下の加熱で二酸化炭素を回収でき、且つ成形性や加工性に富んだナトリウムフェライト粒子粉末、並びに該粒子粉末の製造方法を提供する。【解決手段】Al、Ga、In、Cr、Mn、Co、Rh、Sc、Y及びCeからなる3価金属群より選ばれた少なくとも1種類以上の金属が、固溶、または、特定の結晶形態を持たない状態で、酸化物換算として0.05~5重量%存在し、Na/Feのモル比が0.75~1.25であることを特徴とするナトリウムフェライト粒子粉末である。【選択図】なし